Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 30.5 kJ/m² | 14.5 ft-lb/in² | ISO 180 |
LNP Thermocomp® UF-1006 A HS Polyphthalamide, Glass Fiber Reinforcement
(discontinued **) Features: Heat StabilizedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are sti.. |