Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 2.20 kJ/m² | 1.05 ft-lb/in² | ASTM D256 |
Tipco Tipcolite® THD 311 Phenolic Compound, Wood Flour, having Medium Flow & High Strength Medium Flow Phenolic Compound, Reinforced with Wood FlourApplications: Electrical & ElectronicsProcessing: Compression MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India... |
|||
Izod Impact, Unnotched (ISO) | 2.20 kJ/m² | 1.05 ft-lb/in² | ASTM D256 |
Tipco Tipcolite® THR 211 Phenolic Compound, Asbestos Wood Flour & Minerals, Soft Flow & High Electrical Properties Soft Flow Phenolic Compound, Reinforced with Asbestos Wood Flour & MineralsApplications: Switchgear, HRC FusesProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industrie.. |
|||
Izod Impact, Unnotched (ISO) | 2.20 kJ/m² | 1.05 ft-lb/in² | ASTM D256 |
Tipco Tipcolite® TX 211 Phenolic Compound, Wood Flour, having Medium Flow & High Electrical Properties Medium Flow Phenolic Compound, Reinforced with Wood FlourApplications: Switchgear, HRC FusesProcessing: Compression MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Izod Impact, Unnotched (ISO) | 2.20 kJ/m² | 1.05 ft-lb/in² | ASTM D256 |
Tipco Tipcolite® TX 311 Phenolic Compound, Wood Flour & Minerals, having Soft Flow & High Strength Soft Flow Phenolic Compound, Reinforced with Wood Flour & MineralsApplications: Switchgear, HRC FusesProcessing: Injection MouldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
I.. |
|||
Izod Impact, Unnotched (ISO) | 2.20 kJ/m² | 1.05 ft-lb/in² | ASTM D256 |
Tipco Tipcolite® TX 312 Phenolic Compound, Wood Flour & Minerals having Soft Flow & Lower Density Soft Flow Phenolic Compound, Reinforced with Wood Flour & MineralsApplications: Switchgear, HRC FusesProcessing: Injection MouldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
I.. |