Polymer Property : Izod Impact, Unnotched (ISO) = 68.5 kJ/m² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched (ISO) 41.0 - 68.5 kJ/m²
19.5 - 32.6 ft-lb/in²
Average value: 55.2 kJ/m² Grade Count:4
Overview of materials for Nylon 66, Carbon Fiber/PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Carbon Fiber/PTFE Filled". Each property range of values reported is minimum and maximum value..