Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 40.0 - 68.0 kJ/m² | 19.0 - 32.4 ft-lb/in² | Average value: 50.7 kJ/m² Grade Count:13 |
Overview of materials for Polyphthalamide (PPA), 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are.. |
|||
Izod Impact, Unnotched (ISO) | 18.0 - 68.0 kJ/m² @Temperature -45.0 - -30.0 °C |
8.57 - 32.4 ft-lb/in² @Temperature -49.0 - -22.0 °F |
Average value: 42.8 kJ/m² Grade Count:6 |
Overview of materials for Polypropylene with 30% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Glass Fiber Filler". Specific grades with glass content between 25% and 34% are i.. |