Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 20.0 - 20.0 kJ/m² @Temperature -30.0 - -30.0 °C |
9.52 - 9.52 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 20.0 kJ/m² Grade Count:1 |
Overview of materials for Polystyrene, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Impact Modified". Each property range of values reported is minimum and maximum values of a.. |
|||
Izod Impact, Unnotched (ISO) | 20.0 - 20.0 kJ/m² @Temperature -30.0 - -30.0 °C |
9.52 - 9.52 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 20.0 kJ/m² Grade Count:1 |
Overview of materials for Polystyrene + Polyphenylene Ether, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene + Polyphenylene Ether, Unreinforced". Each property range of values reported is minimum and .. |
|||
Izod Impact, Unnotched (ISO) | 18.0 - 20.0 kJ/m² | 8.57 - 9.52 ft-lb/in² | Average value: 19.3 kJ/m² Grade Count:3 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled". Specific grades with glass content betwe.. |
|||
Izod Impact, Unnotched (ISO) | 15.0 - 20.0 kJ/m² | 7.14 - 9.52 ft-lb/in² | Average value: 17.7 kJ/m² Grade Count:3 |
Overview of materials for Polypropylene with 20% Calcium Carbonate (CaCO3) Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Calcium Carbonate (CaCO3) Filler". Each property range of values reported is mini.. |
|||
Izod Impact, Unnotched (ISO) | 20.0 - 20.0 kJ/m² @Temperature -30.0 - -30.0 °C |
9.52 - 9.52 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 20.0 kJ/m² Grade Count:2 |
Overview of materials for Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled". Specific grades with glass content between 35% an.. |
|||
Izod Impact, Unnotched (ISO) | 8.00 - 20.0 kJ/m² | 3.81 - 9.52 ft-lb/in² | Average value: 16.0 kJ/m² Grade Count:3 |
Overview of materials for High Density Polyethylene (HDPE), Injection Molded This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Injection Molded". Each property range of values reported is minimum a.. |
|||
Izod Impact, Unnotched (ISO) | 10.0 - 20.0 kJ/m² | 4.76 - 9.52 ft-lb/in² | Average value: 16.0 kJ/m² Grade Count:3 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Stainless Steel Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Stainless Steel Fiber Filled". Each property range of values repo.. |