Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 6.00 - 16.0 kJ/m² | 2.86 - 7.61 ft-lb/in² | Spec; ISO 180 |
Axion Polymers Axpoly® PS02 Impact Modified Polystyrene 100% post-consumer recycled polymer (recovered from television casings)93% less CO2 impact compared with virgin*Successfully replaces virgin grade resinISO9000 quality certifiedAvailable in black/gr.. |
|||
Izod Impact, Unnotched (ISO) | 6.00 - 16.0 kJ/m² | 2.86 - 7.61 ft-lb/in² | Spec; ISO 180 |
Axion Polymers Axpoly® PS13 Impact Modified Polystyrene 100% post-consumer recycled polymer (recovered from coat hangers)93% less CO2 impact compared with virgin*Successfully replaces virgin grade resinISO9000 quality certifiedAvailable in black/greyCost.. |
|||
Izod Impact, Unnotched (ISO) | 12.0 - 16.0 kJ/m² | 5.71 - 7.61 ft-lb/in² | Spec; ISO 180 |
Axion Polymers Axpoly® PS13 1011 High Impact Polystyrene PS13 Series polystyrenes offers the designer and processor a high performance polymer with well-defined properties in a range of options to suit many applications.The Axpoly® PS13 range of resin co.. |