Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 55.0 - 105 kJ/m² | 26.2 - 50.0 ft-lb/in² | Average value: 77.5 kJ/m² Grade Count:16 |
Overview of materials for Nylon 66, 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. .. |
|||
Izod Impact, Unnotched (ISO) | 50.0 - 105 kJ/m² @Temperature -40.0 - -30.0 °C |
23.8 - 50.0 ft-lb/in² @Temperature -40.0 - -22.0 °F |
Average value: 73.8 kJ/m² Grade Count:9 |
Overview of materials for Nylon 66, 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. .. |