Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 8.00 kJ/m² | 3.81 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP BX03658N SAN LNP* LUBRICOMP* BX03658N is a compound based on SAN resin containing proprietary fillers. Added features of this grade include: Wear Resistant, Tight Dimensional Tolerances, good for Water Meter A.. |
|||
Izod Impact, Unnotched (ISO) | 8.00 kJ/m² - NB | 3.81 ft-lb/in² - NB | Average value: 57.3 kJ/m² Grade Count:30 |
Overview of materials for Nylon 12 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12". Each property range of values reported is minimum and maximum values of appropriate MatWeb en.. |
|||
Izod Impact, Unnotched (ISO) | 8.00 kJ/m² | 3.81 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP STAT-KON MX01739C PP LNP* SAT-KON* MX01739C is a compound based on Polypropylene containing Proprietary Filler(s). Added features of this grade include: Electrically Conductive, Clean Compounding System. |
|||
Izod Impact, Unnotched (ISO) | 8.00 kJ/m² @Temperature 23.0 °C |
3.81 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Stat-kon PE002 PA 6 LNP* Stat-kon* PE002 is a compound based on Nylon 6 resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the Americ.. |
|||
Izod Impact, Unnotched (ISO) | 8.00 kJ/m² @Temperature 23.0 °C |
3.81 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Stat-kon PE002 PA 6 (Asia Pacific) LNP* Stat-kon* PE002 is a compound based on Nylon 6 resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the Asia P.. |
|||
Izod Impact, Unnotched (ISO) | 8.00 kJ/m² | 3.81 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP MH0400A PP (Asia Pacific) LNP THERMOCOMP* MH0400A is a compound based on Polypropylene resin. Added features of this material include: High Specific Gravity. |
|||
Izod Impact, Unnotched (ISO) | 8.00 kJ/m² @Temperature 23.0 °C |
3.81 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Thermocomp MH0500A PP (Asia Pacific) LNP THERMOCOMP* MH0500A is a compound based on Polypropylene resin. Added features of this material include: High Specific Gravity.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Unnotched (ISO) | 8.00 kJ/m² | 3.81 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP MF006AL PP LNP* THERMOCOMP* MF006AL is a compound based on Polypropylene resin containing 30% Glass Fiber. Characteristics of this grade are: Low Extractable. |
|||
Izod Impact, Unnotched (ISO) | 8.00 kJ/m² @Temperature 23.0 °C |
3.81 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Thermocomp MH0255A PP (Europe-Africa-Middle East) LNP* THERMOCOMP* MH0255A is a compound based on Polypropylene resin containing Proprietary Filler(s). Added features include; High Specific Gravity.This data was supplied by SABIC-IP for the Europe-.. |
|||
Izod Impact, Unnotched (ISO) | 8.00 kJ/m² | 3.81 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP MH0400A PP LNP THERMOCOMP* MH0400A is a compound based on Polypropylene resin. Added features of this material include: High Specific Gravity. |
|||
Izod Impact, Unnotched (ISO) | 8.00 kJ/m² | 3.81 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOTUF CF007IXP PS LNP* Thermotuf* CF007IXP is a compound based on Polystyrene containing glass fiber. Characteristics of this grade are: High Impact. |
|||
Izod Impact, Unnotched (ISO) | 8.00 kJ/m² | 3.81 ft-lb/in² | ISO 180 |
Polyram PlusTek PD1002NT Nylon 12 for Extrusion Medium viscosity Nylon 12 for extrusion application.Information provided by Polyram. |
|||
Izod Impact, Unnotched (ISO) | 8.00 kJ/m² | 3.81 ft-lb/in² | |
Goodfellow TPX® DX231 Coating/Extrusion Grade Polymethylpentene This grade is highly recommended for paper coating or for fiber extrusion.TPX® is semi-crystalline, transparent, very light and - for a polyolefin - expensive. It has good release characteristics a.. |
|||
Izod Impact, Unnotched (ISO) | 8.00 kJ/m² | 3.81 ft-lb/in² | 80x10x4; ISO 180/1U |
Eurostar Starpylen HZ 80E7 HDPE, Injection Molding Starpylen HZ 80E7 is a High Specific Gravity Polypropylene, Injection Molding ResinInformation provided by Eurostar. |
|||
Izod Impact, Unnotched (ISO) | 8.00 kJ/m² | 3.81 ft-lb/in² | ISO 180/1C |
Chi Mei Polyrex® PG-80N Polystyrene High strength |
|||
Izod Impact, Unnotched (ISO) | 8.00 kJ/m² | 3.81 ft-lb/in² | Typical; ISO 180 |
Axion Polymers Axpoly® PS01 3003 Enhanced White General Purpose Polystyrene PS01 Series polystyrenes offers the designer and processor a high performance polymer with well-defined properties in a range of options to suit many applications.The Axpoly® PS01 range of resin co.. |
|||
Izod Impact, Unnotched (ISO) | 8.00 kJ/m² | 3.81 ft-lb/in² | Typical; ISO 180 |
Axion Polymers Axpoly® PS01 3009 Green General Purpose Polystyrene PS01 Series polystyrenes offers the designer and processor a high performance polymer with well-defined properties in a range of options to suit many applications.The Axpoly® PS01 range of resin co.. |
|||
Izod Impact, Unnotched (ISO) | 8.00 kJ/m² | 3.81 ft-lb/in² | Typical; ISO 180 |
Axion Polymers Axpoly® PS01 Impact Modified Polystyrene 100% post-consumer recycled polymer (recovered from refrigerators)93% less CO2 impact compared with virgin*Successfully replaces virgin grade resinISO9000 quality certifiedAvailable in a range of co.. |
|||
Izod Impact, Unnotched (ISO) | 8.00 kJ/m² | 3.81 ft-lb/in² | Typical; ISO 180 |
Axion Polymers Axpoly® PS02 1000 General Purpose Polystyrene PS02 Series polystyrenes offer the designer and processor a high performance polymer with well-defined properties in a range of options to suit many applications.The Axpoly® PS02 range of resin com.. |
|||
Izod Impact, Unnotched (ISO) | 8.00 - 12.0 kJ/m² | 3.81 - 5.71 ft-lb/in² | Spec; ISO 180 |
Axion Polymers Axpoly® PS02 1010 Medium Impact Polystyrene PS02 Series polystyrenes offers the designer and processor a high performance polymer with well-defined properties in a range of options to suit many applications.The Axpoly® PS02 range of resin co.. |
|||
Izod Impact, Unnotched (ISO) | 8.00 - 14.0 kJ/m² | 3.81 - 6.66 ft-lb/in² | Typical; ISO 180 |
Axion Polymers Axpoly® PS02 Impact Modified Polystyrene 100% post-consumer recycled polymer (recovered from television casings)93% less CO2 impact compared with virgin*Successfully replaces virgin grade resinISO9000 quality certifiedAvailable in black/gr.. |
|||
Izod Impact, Unnotched (ISO) | 8.00 kJ/m² | 3.81 ft-lb/in² | Typical; ISO 180 |
Axion Polymers Axpoly® PS13 1000 Impact Modified Polystyrene PS13 Series polystyrenes offers the designer and processor a high performance polymer with well-defined properties in a range of options to suit many applications.The Axpoly® PS13 range of resin co.. |
|||
Izod Impact, Unnotched (ISO) | 8.00 - 14.0 kJ/m² | 3.81 - 6.66 ft-lb/in² | Typical; ISO 180 |
Axion Polymers Axpoly® PS13 Impact Modified Polystyrene 100% post-consumer recycled polymer (recovered from coat hangers)93% less CO2 impact compared with virgin*Successfully replaces virgin grade resinISO9000 quality certifiedAvailable in black/greyCost.. |
|||
Izod Impact, Unnotched (ISO) | 8.00 kJ/m² | 3.81 ft-lb/in² | Typical; ISO 180 |
Axion Polymers Axpoly® PS01 3000 General Purpose Polystyrene PS01 Series polystyrenes offer the designer and processor a high performance polymer with well-defined properties in a range of options to suit many applications.The Axpoly® PS01 range of custom co.. |
|||
Izod Impact, Unnotched (ISO) | 8.00 - 20.0 kJ/m² | 3.81 - 9.52 ft-lb/in² | Average value: 16.0 kJ/m² Grade Count:3 |
Overview of materials for High Density Polyethylene (HDPE), Injection Molded This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Injection Molded". Each property range of values reported is minimum a.. |
|||
Izod Impact, Unnotched (ISO) | 8.00 - 129 kJ/m² | 3.81 - 61.4 ft-lb/in² | Average value: 43.0 kJ/m² Grade Count:7 |
Overview of materials for Polymethylpentene, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polymethylpentene, Molded". Each property range of values reported is minimum and maximum values of appr.. |
|||
Izod Impact, Unnotched (ISO) | 8.00 kJ/m² | 3.81 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP STAT-KON ME003S PP LNP* STAT-KON* ME003S is a compound based on Polypropylene resin containing 15% Carbon Fiber. Added features of this material include: Electrically Conductive, Heat Stabilized. |