Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 75.0 kJ/m² | 35.7 ft-lb/in² | DIN 53453 |
Ineos Nova S-4400 High Impact Compact Polystyrene
(discontinued **) Impact polystyrene which combines excellent flow characteristics with a good dimensional stability under heat and a high stiffness. This grade is designed for injection molding of technical parts o.. |
|||
Izod Impact, Unnotched (ISO) | 75.0 kJ/m² - NB @Temperature -30.0 - -30.0 °C |
35.7 ft-lb/in² - NB @Temperature -22.0 - -22.0 °F |
Average value: 88.7 kJ/m² Grade Count:10 |
Overview of materials for Nylon 6, 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. E.. |
|||
Izod Impact, Unnotched (ISO) | 75.0 - 85.0 kJ/m² @Temperature -30.0 - -30.0 °C |
35.7 - 40.4 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 80.0 kJ/m² Grade Count:2 |
Overview of materials for Nylon 6, 40% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Mineral Filled". Each property range of values reported is minimum and maximum values of ap.. |
|||
Izod Impact, Unnotched (ISO) | 75.0 kJ/m² | 35.7 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP RFN18SXS PA 66 (Europe-Africa-Middle East) LNP* Lubricomp* RFN18SXS is a compound based on Nylon 66 resin containing Glass Fiber, MOS2. Added features of this material include: Heat Stabilized. |
|||
Izod Impact, Unnotched (ISO) | 75.0 kJ/m² | 35.7 ft-lb/in² | ISO 180 |
Solvay Specialty Polymers Omnix® FC-9050 Polyamide, High Performance (HPPA), 50% Glass Fiber Omnix® FC-9050 is a 50% glass-fiber reinforced high-performance polyamide. It is hot-water moldable and intended for use in components requiring superior mechanical properties even after moisture.. |
|||
Izod Impact, Unnotched (ISO) | 75.0 kJ/m² | 35.7 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP HF004 PA 11 LNP* Thermocomp* HF004 is a compound based on Nylon 11 resin containing 20% Glass Fiber. |
|||
Izod Impact, Unnotched (ISO) | 75.0 kJ/m² | 35.7 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP HF008 PA 11 (Asia Pacific) LNP* THERMOCOMP* HF008 is a compound based on Nylon 11 resin containing Glass Fiber. |
|||
Izod Impact, Unnotched (ISO) | 75.0 kJ/m² | 35.7 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP HX03409C PA11 LNP* THERMOCOMP* HX03409C is a compound based on Nylon 11 resin containing Proprietary Filler(s). Added features of this material include: Clean Compound System, High Specific Gravity. |
|||
Izod Impact, Unnotched (ISO) | 75.0 kJ/m² | 35.7 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP PF1006HI005 PA 6 (Europe-Africa-Middle East) High Impact Nylon 6 compound containing Glass Fiber. |
|||
Izod Impact, Unnotched (ISO) | 75.0 kJ/m² @Temperature -30.0 °C |
35.7 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP PF1006HI005 PA 6 (Europe-Africa-Middle East) High Impact Nylon 6 compound containing Glass Fiber. |
|||
Izod Impact, Unnotched (ISO) | 75.0 kJ/m² | 35.7 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP RF006I PA 66 LNP* THERMOTUF* RF006I is a compound based on Nylon 66 resin containing 30% Glass Fiber. Added features of this material include: High Impact. |
|||
Izod Impact, Unnotched (ISO) | 75.0 kJ/m² | 35.7 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP RF006S PA6.6 (Europe-Africa-Middle East) LNP* THERMOCOMP* RF006S is a compound based on PA 66 resin containing Glass Fiber. Added features include: Heat Stabilized. |
|||
Izod Impact, Unnotched (ISO) | 75.0 kJ/m² | 35.7 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP RF00C PA 66 (Europe-Africa-Middle East) LNP* Thermocomp* RF00C is a compound based on Nylon 66 resin containing Glass Fiber. |
|||
Izod Impact, Unnotched (ISO) | 75.0 kJ/m² @Temperature 23.0 °C |
35.7 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Thermocomp RX06423 PA 66 LNP* Thermocomp* RX06423 is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, UV Stabilized.This data was supplied b.. |
|||
Izod Impact, Unnotched (ISO) | 75.0 kJ/m² | 35.7 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP RX12402 PA 66 LNP* Thermocomp* RX12402 is a compound based on PA66 containing 60% Glass Fiber. Added feature is Superior Flow. |
|||
Izod Impact, Unnotched (ISO) | 75.0 kJ/m² | 35.7 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP DB0049R PC (Europe-Africa-Middle East) LNP* Thermocomp* DB0049R is a compound based on Polycarbonate resin containing Glass Bead, Flame Retardant. Added features of this material include: Flame Retardant. |
|||
Izod Impact, Unnotched (ISO) | 75.0 kJ/m² | 35.7 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP HF008 PA11 LNP THERMOCOMP* HF008 is a compound based on Nylon 11 resin containing 40% Glass Fiber. |
|||
Izod Impact, Unnotched (ISO) | 75.0 kJ/m² | 35.7 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP QF00A PA6.10 LNP* THERMOCOMP* QF00A is a compound based on Nylon 6/10 containing 50% Glass Fiber. |
|||
Izod Impact, Unnotched (ISO) | 75.0 kJ/m² @Temperature 23.0 °C |
35.7 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Thermocomp RF007S PA 66 (Europe-Africa-Middle East) LNP* THERMOCOMP* RF007S is a compound based on PA 66 resin containing Glass Fiber . Added features include: Heat Stabilized.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regi.. |
|||
Izod Impact, Unnotched (ISO) | 75.0 kJ/m² | 35.7 ft-lb/in² | ASTM D256 |
Tipco Tipcofil® AM 300 - 15% Mineral Reinforced Nylon-6 Compound, with High Heat Stability 15% Mineral Reinforced Nylon-6 CompoundApplications: General PurposeProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Izod Impact, Unnotched (ISO) | 75.0 kJ/m² | 35.7 ft-lb/in² | DAM; ISO 180/1U |
DuPont Performance Polymers Zytel® 73G30T BK261 Nylon 6
(Unverified Data**) 30% Glass Reinforced Toughened Polyamide 6 Zytel 73G30T BK261 is a 30% glass fiber reinforced toughened black polyamide 6 resin for injection molding.Information provided by DuPont Performance Polym.. |
|||
Izod Impact, Unnotched (ISO) | 75.0 kJ/m² | 35.7 ft-lb/in² | 50%RH; ISO 180/1U |
DuPont Performance Polymers Zytel® 73G30T BK261 Nylon 6
(Unverified Data**) 30% Glass Reinforced Toughened Polyamide 6 Zytel 73G30T BK261 is a 30% glass fiber reinforced toughened black polyamide 6 resin for injection molding.Information provided by DuPont Performance Polym.. |
|||
Izod Impact, Unnotched (ISO) | 75.0 kJ/m² @Temperature -30.0 °C |
35.7 ft-lb/in² @Temperature -22.0 °F |
50%RH; ISO 180/1U |
DuPont Performance Polymers Zytel® 80G33L NC010 Nylon 66
(Unverified Data**) 33% Glass Reinforced Toughened Polyamide 66 Zytel 80G33L NC010 is a 33% glass fiber reinforced polyamide 66 resin with outstanding impact resistance developed using DuPont Super Tough technology.Inf.. |
|||
Izod Impact, Unnotched (ISO) | 75.0 kJ/m² | 35.7 ft-lb/in² | 80x10x4; ISO 180/1U |
Eurostar Staramide RF007S PA66, 35% Glass Fiber Filled, Injection Molded Staramide RF007S is a 35% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Eurostar. |
|||
Izod Impact, Unnotched (ISO) | 75.0 kJ/m² @Temperature 23.0 °C |
35.7 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1U |
Eurotec® Tecolen® CP20 MF20 NL XC30 PPCP, 20% mineral filled, flame retardant - halogen (RoHS compliant), heat stabilized, natural Information provided by Eurotec® |
|||
Izod Impact, Unnotched (ISO) | 75.0 kJ/m² | 35.7 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP SF008 PA 12 (Asia Pacific) LNP* Thermocomp* SF008 is a compound based on Nylon 12 resin containing Glass Fiber. |
|||
Izod Impact, Unnotched (ISO) | 75.0 kJ/m² @Temperature 23.0 °C |
35.7 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Verton RX93407D PA 66 LNP* Verton* RX93407D is a compound based on Nylon 66 resin.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Unnotched (ISO) | 75.0 kJ/m² @Temperature 23.0 °C |
35.7 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Verton UX06451 PPA LNP* Verton* UX06451 is a compound based on Polyphthalamide resin containing Long Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Unnotched (ISO) | 75.0 kJ/m² | 35.7 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP VERTON UX06451 PPA (Europe-Africa-Middle East) LNP* Verton* UX06451 is a compound based on Polyphthalamide resin containing Long Glass Fiber. |
|||
Izod Impact, Unnotched (ISO) | 75.0 kJ/m² - NB | 35.7 ft-lb/in² - NB | Average value: 94.5 kJ/m² Grade Count:25 |
Overview of materials for Nylon 6, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Impact Grade". Each property range of values reported is minimum and maximum values of appropri.. |