Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 70.0 kJ/m² | 33.3 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP FARADEX NX07330 PC+ABS (Asia Pacific) Faradex NX07330 is a compound based on PC+ABS blend resin containing stainless steel and glass fiber. Added features of this material include EMI/RFI Shielding and ESD. |
|||
Izod Impact, Unnotched (ISO) | 70.0 kJ/m² | 33.3 ft-lb/in² | DIN 53453 |
Ineos Nova S-5400 High Impact Compact Polystyrene
(discontinued **) Impact polystyrene with high dimensional stability under heat, particularly suitable fore extrusion and thermoforming of technical parts or packaging applications but also used for injection molding.. |
|||
Izod Impact, Unnotched (ISO) | 70.0 kJ/m² - NB | 33.3 ft-lb/in² - NB | Average value: 70.0 kJ/m² Grade Count:9 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant". Each property range of values rep.. |
|||
Izod Impact, Unnotched (ISO) | 70.0 kJ/m² - NB | 33.3 ft-lb/in² - NB | Average value: 89.9 kJ/m² Grade Count:19 |
Overview of materials for Nylon 6, 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. E.. |
|||
Izod Impact, Unnotched (ISO) | 70.0 kJ/m² | 33.3 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP GL003XXP PSU (Europe-Africa-Middle East) LNP* LUBRICOMP* GL003XXP is a compound based on Polysulfone resin containing PTFE. Added features include; Internally Lubricated. |
|||
Izod Impact, Unnotched (ISO) | 70.0 kJ/m² | 33.3 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP IFL36R PA6.12 (Europe-Africa-Middle East) Internally lubricated PA6.12, containing Glass Fiber and PTFE |
|||
Izod Impact, Unnotched (ISO) | 70.0 kJ/m² | 33.3 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP RFL36SXC PA 66 (Europe-Africa-Middle East) LNP* Lubricomp* RFL36SXC is a compound based on Nylon 66 resin containing Glass Fiber, PTFE. Added features of this material include: Heat Stabilized. |
|||
Izod Impact, Unnotched (ISO) | 70.0 kJ/m² @Temperature 23.0 °C |
33.3 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Lubricomp RFL38 PA 66 (Europe-Africa-Middle East) LNP* Lubricomp* RFL38 is a compound based on Nylon 66 resin containing Glass Fiber, PTFE.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Unnotched (ISO) | 70.0 kJ/m² | 33.3 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP UFL36S PPA LNP LUBRICOMP* UFL36S is a compound based on Polyphthalamide resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Heat Stabilized, Wear Resistant, Bearing Grade. |
|||
Izod Impact, Unnotched (ISO) | 70.0 kJ/m² | 33.3 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP UFL36SXC PPA LNP* LUBRICOMP* UFL36SXC is a compound based on Polyphthalamide resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Wear Resistant, Heat Stabilized. |
|||
Izod Impact, Unnotched (ISO) | 70.0 kJ/m² | 33.3 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP UFL36SXC PPA (Asia Pacific) LNP* Lubricomp* UFL36SXC is a compound based on Polyphthalamide resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated, Heat Stabilized. |
|||
Izod Impact, Unnotched (ISO) | 70.0 kJ/m² | 33.3 ft-lb/in² | ISO 180 |
Solvay Specialty Polymers AvaSpire® AV-621 GF30 Polyaryletherketone (PAEK), 30% Glass Fiber AvaSpire® AV-621 GF30 is a 30% glass fiber reinforced version of AvaSpire® AV-621. This formulation offers better dimensional stability and lower warpage than 30% glass reinforced PEEK. This r.. |
|||
Izod Impact, Unnotched (ISO) | 70.0 kJ/m² | 33.3 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP STAT-KON DD0009 PC LNP* STAT-KON* DD0009 is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Electrically Conductive, Flame Retardant. |
|||
Izod Impact, Unnotched (ISO) | 70.0 kJ/m² | 33.3 ft-lb/in² | ISO 180 |
Solvay Specialty Polymers Kalix® 3950 Polyamide, High Performance (HPPA), 50% Glass Fiber Kalix® 3950 is a 16% bio-sourced, amorphous polyphthalamide (PPA)-based compound with 50% by weight glass fiber reinforcement. This material is uniquely formulated to prevent warpage and flash in.. |
|||
Izod Impact, Unnotched (ISO) | 70.0 kJ/m² | 33.3 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP RC008ESS PA 66 (Europe-Africa-Middle East) LNP* THERMOCOMP* RC008ESS is a compound based on PA66 resin containing Carbon Fiber. Added features include; Electrically Conductive, Easy Molding, Heat Stabilized. |
|||
Izod Impact, Unnotched (ISO) | 70.0 kJ/m² @Temperature 23.0 °C |
33.3 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Thermotuf PK005EI2 PA 6 (Europe-Africa-Middle East) LNP* THERMOTUF* PK005EI2 is a compound based on PA 6 resin containing Impact Modifier, Mineral. Added features include: High Impact.This data was supplied by SABIC-IP for the Europe-Africa-Middle Ea.. |
|||
Izod Impact, Unnotched (ISO) | 70.0 kJ/m² | 33.3 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP VERTON RV008ES PA 66 LNP* VERTON* RV008ES is a compound based on Nylon 66 resin containing 40% Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, Structural. |
|||
Izod Impact, Unnotched (ISO) | 70.0 kJ/m² | 33.3 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP VERTON RV008ES PA 66 (Asia Pacific) LNP* Verton* RV008ES is a compound based on Nylon 66 resin containing Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized. |
|||
Izod Impact, Unnotched (ISO) | 70.0 kJ/m² | 33.3 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP VERTON RX02059 PA 66 (Europe-Africa-Middle East) LNP* VERTON* RX02059 is a compound based on PA 66 resin containing Long Glass Fiber, Proprietary Lubricant. Added features include; Internally Lubricated. |
|||
Izod Impact, Unnotched (ISO) | 70.0 kJ/m² | 33.3 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP VERTON RX03013 PA 66 (Europe-Africa-Middle East) LNP* VERTON* RX03013 is a compound based on PA 66 resin containing Long Glass Fiber, Proprietary Lubricant. Added features include: Internally Lubricated. |
|||
Izod Impact, Unnotched (ISO) | 70.0 kJ/m² | 33.3 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP VERTON UX03320 PPA (Europe-Africa-Middle East) VERTON* UX03320 is a compound based on Polyphthalamide resin containing Long Glass. |
|||
Izod Impact, Unnotched (ISO) | 70.0 kJ/m² @Temperature -30.0 °C |
33.3 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1U |
DuPont Performance Polymers Crastin® S620F20 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l Unreinforced Medium Viscosity Polybutylene Terephthalate Crastin S620F20 NC010 is an unreinforced nucleated lubricated medium viscosity polybutylene terephthalate resin for fast injection molding.In.. |
|||
Izod Impact, Unnotched (ISO) | 70.0 kJ/m² @Temperature -30.0 °C |
33.3 ft-lb/in² @Temperature -22.0 °F |
50%RH; ISO 180/1U |
DuPont Performance Polymers Zytel® 8018HS NC010 Nylon 66
(Unverified Data**) 14% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 8018HS NC010 is a 14% glass reinforced heat stabilized toughened polyamide 66 resin.Information provided by DuPont Performance Polym.. |
|||
Izod Impact, Unnotched (ISO) | 70.0 kJ/m² | 33.3 ft-lb/in² | 80x10x4; ISO 180/1U |
Eurostar Star L PA6 30V D51 PA6, Glass Filled, Injection Molding Star L PA6 30V D51 is a PTFE Lubricated, Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Izod Impact, Unnotched (ISO) | 70.0 kJ/m² | 33.3 ft-lb/in² | 80x10x4; ISO 180/1U |
Eurostar Staramide RF008U PA66/6, 40% Glass Filled, Injection Molded Staramide RF008U is a 40% Glass Fiber Reinforced Polyamide 66/Polyamide 6 Injection Molding Resin (also known as Staramide 66 C 40V S4)Information provided by Eurostar. |
|||
Izod Impact, Unnotched (ISO) | 70.0 kJ/m² | 33.3 ft-lb/in² | 80x10x4; ISO 180/1U |
Eurostar Starpylen MK001AS PP, Mineral Filled, Injection Molding Starpylen MK001AS is a Mineral Filled Polypropylene Injection Molding ResinInformation provided by Eurostar. |
|||
Izod Impact, Unnotched (ISO) | 70.0 kJ/m² | 33.3 ft-lb/in² | ASTM D256 |
Beijing Ranger Chem PBT 403 G-M50 Heat Resistant and Environmental Protection Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Izod Impact, Unnotched (ISO) | 70.0 - 70.0 kJ/m² @Temperature -30.0 - -30.0 °C |
33.3 - 33.3 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 70.0 kJ/m² Grade Count:1 |
Overview of materials for Nylon 66, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, PTFE Filled". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Izod Impact, Unnotched (ISO) | 70.0 kJ/m² | 33.3 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP VERTON RX970079 PA 66 (Europe-Africa-Middle East) LNP* VERTON* RX970079 is a compound based on PA 66 resin containing Long Glass Fiber and PTFE. Added features include; Internally Lubricated. |
|||
Izod Impact, Unnotched (ISO) | 70.0 kJ/m² | 33.3 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP VERTON UX03320 PPA (Asia Pacific) VERTON* UX03320 is a compound based on Polyphthalamide resin containing Long Glass. |