Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 6.00 kJ/m² | 2.86 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP KONDUIT OX11314 PPS (Europe-Africa-Middle East) Thermally conductive mineral and glass fiber filled PPS Eco-FR compound |
|||
Izod Impact, Unnotched (ISO) | >= 6.00 kJ/m² | >= 2.86 ft-lb/in² | ISO 180/1A |
Iran Petrochemical (PCC) Tabriz 4240/1 High Impact Polystyrene
(discontinued **) Information provided by Iran Petrochemical Commercial Co. |
|||
Izod Impact, Unnotched (ISO) | 6.00 kJ/m² | 2.86 ft-lb/in² | DIN 53453 |
Ineos Nova S-7600MG Compact Polystyrene Microgranulates
(discontinued **) High impact polystyrene Microgranulates, having a diameter of 0.8 -1.0 mm, especially useful for compounding and extrusion applications. Due to the very high viscosity and the absence of weakener, .. |
|||
Izod Impact, Unnotched (ISO) | 6.00 kJ/m² | 2.86 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP BX02715 SAN LNP* LUBRICOMP* BX02715 is a compound based on SAN containing proprietary fillers. Added features of this grade include: Wear Resistant, Tight Dimensional Tolerance, Good for Water Meter Applicati.. |
|||
Izod Impact, Unnotched (ISO) | 6.00 kJ/m² | 2.86 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP CF008 PS LNP* THERMOCOMP* CF008 is a compound based on Polystyrene resin containing 40% Glass Fiber. |
|||
Izod Impact, Unnotched (ISO) | 6.00 kJ/m² | 2.86 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP AH0400A ABS LNP* THERMOCOMP* AH0400A is a compound based on ABS resin. Added feature of this material is: High Specific Gravity. |
|||
Izod Impact, Unnotched (ISO) | 6.00 kJ/m² @Temperature 23.0 °C |
2.86 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Thermocomp OF002A PPS LNP* Thermocomp* OF002A is a compound based on Polyphenylene Sulfide resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Unnotched (ISO) | 6.00 kJ/m² @Temperature 23.0 °C |
2.86 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Thermocomp OF002A PPS (Asia Pacific) LNP* Thermocomp* OF002A is a compound based on Polyphenylene Sulfide resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Unnotched (ISO) | 6.00 kJ/m² | 2.86 ft-lb/in² | ISO 180/1C |
Chi Mei Polyrex® PG-22 Polystyrene TPE compound |
|||
Izod Impact, Unnotched (ISO) | 6.00 - 10.0 kJ/m² | 2.86 - 4.76 ft-lb/in² | Spec; ISO 180 |
Axion Polymers Axpoly® PS01 3003 Enhanced White General Purpose Polystyrene PS01 Series polystyrenes offers the designer and processor a high performance polymer with well-defined properties in a range of options to suit many applications.The Axpoly® PS01 range of resin co.. |
|||
Izod Impact, Unnotched (ISO) | 6.00 - 10.0 kJ/m² | 2.86 - 4.76 ft-lb/in² | Spec; ISO 180 |
Axion Polymers Axpoly® PS01 3009 Green General Purpose Polystyrene PS01 Series polystyrenes offers the designer and processor a high performance polymer with well-defined properties in a range of options to suit many applications.The Axpoly® PS01 range of resin co.. |
|||
Izod Impact, Unnotched (ISO) | 6.00 - 10.0 kJ/m² | 2.86 - 4.76 ft-lb/in² | Spec; ISO 180 |
Axion Polymers Axpoly® PS01 Impact Modified Polystyrene 100% post-consumer recycled polymer (recovered from refrigerators)93% less CO2 impact compared with virgin*Successfully replaces virgin grade resinISO9000 quality certifiedAvailable in a range of co.. |
|||
Izod Impact, Unnotched (ISO) | 6.00 - 10.0 kJ/m² | 2.86 - 4.76 ft-lb/in² | Spec; ISO 180 |
Axion Polymers Axpoly® PS02 1000 General Purpose Polystyrene PS02 Series polystyrenes offer the designer and processor a high performance polymer with well-defined properties in a range of options to suit many applications.The Axpoly® PS02 range of resin com.. |
|||
Izod Impact, Unnotched (ISO) | 6.00 - 16.0 kJ/m² | 2.86 - 7.61 ft-lb/in² | Spec; ISO 180 |
Axion Polymers Axpoly® PS02 Impact Modified Polystyrene 100% post-consumer recycled polymer (recovered from television casings)93% less CO2 impact compared with virgin*Successfully replaces virgin grade resinISO9000 quality certifiedAvailable in black/gr.. |
|||
Izod Impact, Unnotched (ISO) | 6.00 - 10.0 kJ/m² | 2.86 - 4.76 ft-lb/in² | Spec; ISO 180 |
Axion Polymers Axpoly® PS13 1000 Impact Modified Polystyrene PS13 Series polystyrenes offers the designer and processor a high performance polymer with well-defined properties in a range of options to suit many applications.The Axpoly® PS13 range of resin co.. |
|||
Izod Impact, Unnotched (ISO) | 6.00 - 16.0 kJ/m² | 2.86 - 7.61 ft-lb/in² | Spec; ISO 180 |
Axion Polymers Axpoly® PS13 Impact Modified Polystyrene 100% post-consumer recycled polymer (recovered from coat hangers)93% less CO2 impact compared with virgin*Successfully replaces virgin grade resinISO9000 quality certifiedAvailable in black/greyCost.. |
|||
Izod Impact, Unnotched (ISO) | 6.00 - 10.0 kJ/m² | 2.86 - 4.76 ft-lb/in² | Spec; ISO 180 |
Axion Polymers Axpoly® PS01 3000 General Purpose Polystyrene PS01 Series polystyrenes offer the designer and processor a high performance polymer with well-defined properties in a range of options to suit many applications.The Axpoly® PS01 range of custom co.. |
|||
Izod Impact, Unnotched (ISO) | 6.00 kJ/m² @Temperature 23.0 °C |
2.86 ft-lb/in² @Temperature 73.4 °F |
ISO 180/U |
Victrex® PEEK 450GL15 Polyetheretherketone, 15% Glass Fibre Reinforced Product Description:High performance thermoplastic material, 15% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, F.. |