Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 41.0 kJ/m² | 19.5 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP DAL22 PC LNP* Lubricomp* DAL22 is a compound based on Polycarbonate resin containing 10% PTFE and 10% Aramid Fiber. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Unnotched (ISO) | 41.0 kJ/m² | 19.5 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP DAL22 PC (Asia Pacific) LNP* Lubricomp* DAL22 is a compound based on Polycarbonate resin containing PTFE, Aramid Fiber. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Unnotched (ISO) | 41.0 - 70.0 kJ/m² | 19.5 - 33.3 ft-lb/in² | Average value: 61.0 kJ/m² Grade Count:4 |
Overview of materials for Polyaryletherketone (PAEK), Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyaryletherketone (PAEK), Glass Fiber Filled". Each property range of values reported is minimum and m.. |
|||
Izod Impact, Unnotched (ISO) | 41.0 kJ/m² | 19.5 ft-lb/in² | ISO 180 |
Solvay Specialty Polymers AvaSpire® AV-750 GF40 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-750 GF40 is a 40% glass reinforced polyaryletherketone (PAEK) designed to fill the marketplace need for a lower-priced PEEK (polyetheretherketone). This resin provides the typical chemic.. |
|||
Izod Impact, Unnotched (ISO) | 41.0 - 52.0 kJ/m² | 19.5 - 24.7 ft-lb/in² | Average value: 46.3 kJ/m² Grade Count:4 |
Overview of materials for Nylon 66, 10% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Carbon Fiber Filled". Specific grades with carbon fiber content between 5% and 14% are inc.. |
|||
Izod Impact, Unnotched (ISO) | 41.0 - 68.5 kJ/m² | 19.5 - 32.6 ft-lb/in² | Average value: 55.2 kJ/m² Grade Count:4 |
Overview of materials for Nylon 66, Carbon Fiber/PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Carbon Fiber/PTFE Filled". Each property range of values reported is minimum and maximum value.. |
|||
Izod Impact, Unnotched (ISO) | 41.0 kJ/m² | 19.5 ft-lb/in² | |
Idemitsu Kosan Xarec® WA 552 SPS, 30% Glass Filled Crystalline Polymer, Glass Filled/Impact Modified. Used in Automotive and Industrial applications. NSF and medical approval ISO 10993 |
|||
Izod Impact, Unnotched (ISO) | 41.0 kJ/m² | 19.5 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP RAL22I PA 66 LNP* LUBRICOMP* RAL22I is a compound based on Nylon 66 resin containing 10% PTFE, 10% Aramid Fiber. Added features of this material include: Wear Resistant, High Impact. |
|||
Izod Impact, Unnotched (ISO) | 41.0 kJ/m² | 19.5 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP WFL34 PBT LNP LUBRICOMP* WFL34 is a compound based on PBT resin containing 20% Glass Fiber, 15% PTFE. Added feature of this grade is: Wear Resistant. |
|||
Izod Impact, Unnotched (ISO) | 41.0 kJ/m² | 19.5 ft-lb/in² | ISO 180 |
Solvay Specialty Polymers AvaSpire® AV-750 GF40 Polyaryletherketone (PAEK), 40% Glass Fiber AvaSpire® AV-750 GF40 is a 40% glass reinforced polyaryletherketone (PAEK) designed to fill the marketplace need for a lower-priced PEEK (polyetheretherketone). This resin provides the typical ch.. |
|||
Izod Impact, Unnotched (ISO) | 41.0 kJ/m² | 19.5 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP STAT-KON DEF42 PC LNP STAT-KON* DEF42 is a compound based on Polycarbonate resin containing 20% Glass Fiber, 10% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Izod Impact, Unnotched (ISO) | 41.0 kJ/m² @Temperature 23.0 °C |
19.5 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Stat-kon REL36 PA 66 LNP* Stat-Kon* REL36 is a compound based on Nylon 6/6 containing carbon fiber and PTFE. Characteristics of this grade are Statically Conductive.This data was supplied by SABIC-IP for the Americas r.. |
|||
Izod Impact, Unnotched (ISO) | 41.0 kJ/m² | 19.5 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP IX04513C PA 6/12 (Asia Pacific) LNP THERMOCOMP* IX04513C is a compound based on Nylon 6/12 resin containing Glass Fiber. Added features of this material include: Clean Compounding System. |
|||
Izod Impact, Unnotched (ISO) | 41.0 kJ/m² | 19.5 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP KF006XXC Acetal Copolymer LNP* THERMOCOMP* KF006XXC is a compound based on Acetal Copolymer resin containing 30% Glass Fiber. |
|||
Izod Impact, Unnotched (ISO) | 41.0 kJ/m² | 19.5 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP KF006XXC Acetal Copolymer (Asia Pacific) LNP* Thermocomp* KF006XXC is a compound based on Acetal Copolymer resin containing Glass Fiber. |
|||
Izod Impact, Unnotched (ISO) | 41.0 kJ/m² | 19.5 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP RF007ES PA 66 LNP* THERMOCOMP* RF007ES is a compound based on Nylon 66 resin containing 35% Glass Fiber. Added features of this material include: Heat Stabilized, Easy Molding. |
|||
Izod Impact, Unnotched (ISO) | 41.0 kJ/m² | 19.5 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP VERTON NV004E PC+ABS LNP VERTON* NV004E is a compound based on PC+ABS Blend resin containing 20% Long Glass Fiber. Added features of this material include: Easy Molding, Structural. |
|||
Izod Impact, Unnotched (ISO) | 41.0 kJ/m² | 19.5 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP VERTON NV004E PC+ABS (Europe-Africa-Middle East) LNP VERTON* NV004E is a compound based on PC+ABS Blend resin containing Long Glass. Added features of this material include: Easy Molding. |
|||
Izod Impact, Unnotched (ISO) | 41.0 kJ/m² | 19.5 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOTUF VF1001S Super Tough Nylon LNP* Thermotuf* VF1001S is a Super Tough Nylon containing glass fiber. Characteristics of this grade is Heat Stabilized. |
|||
Izod Impact, Unnotched (ISO) | 41.0 kJ/m² | 19.5 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP VERTON NV004E PC+ABS (Asia Pacific) LNP VERTON* NV004E is a compound based on PC+ABS Blend resin containing Long Glass. Added features of this material include: Easy Molding. |
|||
Izod Impact, Unnotched (ISO) | 41.0 kJ/m² | 19.5 ft-lb/in² | 80x10x4; ISO 180/1U |
Eurostar Star L PA66 15Y D52 PA66, Carbon Filled, Injection Molded Star L PA66 15Y D52 is a PTFE Lubricated, Carbon Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Eurostar. |
|||
Izod Impact, Unnotched (ISO) | 41.0 kJ/m² | 19.5 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP IX04513C PA 6/12 LNP THERMOCOMP* IX04513C is a compound based on Nylon 6/12 resin containing Glass Fiber. Added features of this material include: Clean Compounding System. |