Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 34.0 kJ/m² | 16.2 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP DFL32 PC LNP LUBRICOMP* DFL32 is a compound based on Polycarbonate resin containing 10% Glass Fiber and 15% PTFE. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Unnotched (ISO) | 34.0 kJ/m² | 16.2 ft-lb/in² | ISO 180 |
Solvay Specialty Polymers KetaSpire® KT-820 SL30 Polyetheretherketone (PEEK)
(Unverified Data**) Ketaspire KT-820 SL30 is a polyetheretherketone (PEEK) compound designed to provide a balance of excellent mechanical properties, wear resistance and low coefficient of friction in both dry and exte.. |
|||
Izod Impact, Unnotched (ISO) | 34.0 kJ/m² | 16.2 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP LCL33 PEEK LNP* LUBRICOMP* LCL33 is a compound based on Polyetheretherketone resin containing 15% Carbon Fiber, 15% PTFE. Added features of this material include: Wear Resistant. |
|||
Izod Impact, Unnotched (ISO) | 34.0 kJ/m² | 16.2 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP LCL33E PEEK LNP LUBRICOMP* LCL33E is a compound based on Polyetheretherketone resin containing 15% Carbon Fiber, 15% PTFE. Added features of this material include: Easy Molding, Wear Resistant. |
|||
Izod Impact, Unnotched (ISO) | 34.0 kJ/m² | 16.2 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP Lexan_LF0335 PC (Europe-Africa-Middle East) LNP* Lubricomp* LEXAN_LF0335 compound is a 35% glass fiber, milled glass reinforced PC injection moulding resin with improved wear resistance and reduced friction. |
|||
Izod Impact, Unnotched (ISO) | 34.0 kJ/m² | 16.2 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics REMEX VR4831 PBT 15% Glass filled PBT, Flame retardant, UL Recognized, Utility grade, Black color only |
|||
Izod Impact, Unnotched (ISO) | 34.0 kJ/m² @Temperature 23.0 °C |
16.2 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Lubricomp ZFL36CCX PPE+PS LNP LUBRICOMP* ZFL36CCX is a compound based on PPE+PS Blend resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for.. |
|||
Izod Impact, Unnotched (ISO) | 34.0 kJ/m² @Temperature 23.0 °C |
16.2 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Stat-kon DE002P PC LNP STAT-KON* DE002P is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the .. |
|||
Izod Impact, Unnotched (ISO) | 34.0 kJ/m² | 16.2 ft-lb/in² | ISO 180 |
Solvay Specialty Polymers KetaSpire® KT-820 SL30 Polyetheretherketone (PEEK) KetaSpire® KT-820 SL30 is a polyetheretherketone (PEEK) compound designed to provide a balance of excellent mechanical properties, wear resistance and low coefficient of friction in both dry and .. |
|||
Izod Impact, Unnotched (ISO) | 34.0 kJ/m² | 16.2 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP STAT-KON REP349 PA 66 LNP* STAT-KON* REP349 is a compound based on Nylon 66 resin containing 15% PTFE/Silicone, 20% Carbon Fiber. Added features of this material include: Electrically Conductive, Wear Resistant. |
|||
Izod Impact, Unnotched (ISO) | 34.0 kJ/m² | 16.2 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP STAT-KON REP349 PA 66 (Asia Pacific) LNP* Stat-kon* REP349 is a compound based on Nylon 66 resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive, Internally Lubricated. |
|||
Izod Impact, Unnotched (ISO) | 34.0 kJ/m² | 16.2 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP EC006E PEI LNP THERMOCOMP* EC006E is a compound based on Polyetherimide resin containing 30% Carbon Fiber. Added features of this material include: Easy Molding, Electrically Conductive |
|||
Izod Impact, Unnotched (ISO) | 34.0 kJ/m² | 16.2 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP UF00BAS PPA LNP* THERMOCOMP* UF00BAS is a compound based on Polyphthalamide containing 55% Glass Fiber. Added feature of this material is: Heat Stabilized. |
|||
Izod Impact, Unnotched (ISO) | 34.0 kJ/m² | 16.2 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP VERTON E9007E PEI LNP* VERTON* E9007E is a compound based on Polyetherimide (PEI) containing 35% Long Carbon Fiber. Added features of this grade include: Structural, High Temperature |
|||
Izod Impact, Unnotched (ISO) | 34.0 kJ/m² @Temperature -30.0 °C |
16.2 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics NORYL LTA1350 PPE+PS Noryl* LTA1350 is an unfilled, injection moldable grade. Designed for improved long term heat aging, this resin also uses non-chlorinated, non-brominated FR additives to achieve a V0 UL94 rating. No.. |
|||
Izod Impact, Unnotched (ISO) | 34.0 kJ/m² @Temperature -30.0 °C |
16.2 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics NORYL LTA1350 PPE+PS (Asia Pacific) Noryl* LTA1350 is an unfilled, injection moldable grade. Designed for improved long term heat aging, this resin also uses non-chlorinated, non-brominated FR additives to achieve a V0 UL94 rating. No.. |
|||
Izod Impact, Unnotched (ISO) | 34.0 kJ/m² @Temperature -30.0 °C |
16.2 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics NORYL LTA5020 PPE+PS Noryl* LTA5020 is an unfilled, injection moldable grade. Designed for improved long term heat aging, this resin also uses non-chlorinated, non-brominated FR additives to achieve a V0 UL94 rating. No.. |
|||
Izod Impact, Unnotched (ISO) | 34.0 kJ/m² @Temperature 23.0 °C |
16.2 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Stat-kon DE002P PC (Asia Pacific) LNP STAT-KON* DE002P is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the .. |
|||
Izod Impact, Unnotched (ISO) | 34.0 kJ/m² | 16.2 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP STAT-KON DEL22P PC (Asia Pacific) LNP STAT-KON* DEL22P is a compound based on Polycarbonate resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Izod Impact, Unnotched (ISO) | 34.0 kJ/m² | 16.2 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP STAT-LOY WF306C PBT LNP* STAT-LOY* WF306C is a compound based on PBT resin containing 30% Glass Fiber. Added features of this material include: Antistat, Clean Compound System. |
|||
Izod Impact, Unnotched (ISO) | 34.0 kJ/m² | 16.2 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP STAT-LOY WF306C PBT (Asia Pacific) LNP* Stat-loy* WF306C is a compound based on Polybutylene Terephalate resin containing Glass Fiber. Added features of this material include: Antistat, Clean Compounding System. |
|||
Izod Impact, Unnotched (ISO) | 34.0 kJ/m² | 16.2 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP AB002 ABS LNP* THERMOCOMP* AB002 is a compound based on ABS resin containing 10% Glass Bead. |
|||
Izod Impact, Unnotched (ISO) | 34.0 kJ/m² | 16.2 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOTUF VF006U Super Tough Nylon LNP* Thermotuf* VF006U is a compound based on Super Tough Nylon containing Glass Fiber. Characteristics of this grade are High Impact. |
|||
Izod Impact, Unnotched (ISO) | 34.0 kJ/m² @Temperature -30.0 °C |
16.2 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics NORYL LTA1350 PPE+PS (Europe-Africa-Middle East) Noryl* LTA1350 is an unfilled, injection moldable grade. Designed for improved long term heat aging, this resin also uses non-chlorinated, non-brominated FR additives to achieve a V0 UL94 rating. No.. |
|||
Izod Impact, Unnotched (ISO) | >= 34.0 kJ/m² | >= 16.2 ft-lb/in² | Parallel to laminations; IEC 1212-2 5.5.3 |
Hippe EP GC 201 Woven Glass Cloth Reinforced Epoxy Resin - Sheet Used in mechanical, electrical and electronic applications. Extremely high mechanical strength at moderate temperature. Very good stability of electrical properties under high humidity.Information.. |
|||
Izod Impact, Unnotched (ISO) | >= 34.0 kJ/m² | >= 16.2 ft-lb/in² | Parallel to laminations; IEC 1212-2 5.5.3 |
Hippe EP GC 202 Woven Glass Cloth Reinforced Epoxy Resin - Sheet Used in mechanical, electrical and electronic applications. Extremely high mechanical strength at moderate temperature. Very good stability of electrical properties under high humidity. Flame ret.. |
|||
Izod Impact, Unnotched (ISO) | >= 34.0 kJ/m² | >= 16.2 ft-lb/in² | Parallel to laminations; IEC 1212-2 5.5.3 |
Hippe EP GC 204 Woven Glass Cloth Reinforced Epoxy Resin - Sheet Used in mechanical, electrical and electronic applications. Extremely high mechanical strength at moderate temperature. Very good stability of electrical properties under high humidity. High mech.. |
|||
Izod Impact, Unnotched (ISO) | 34.0 kJ/m² | 16.2 ft-lb/in² | 80x10x4; ISO 180/1U |
Eurostar Star L PA66 D51 PA66, Injection Molded Star L PA66 D51 is a PTFE Lubricated, Unreinforced, Polyamide 66 Injection Molding ResinInformation provided by Eurostar. |