Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 20.0 kJ/m² | 9.52 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP FARADEX AS002 ABS LNP* Faradex* AS002 is a compound based on Acrylonitrile Butadiene Styrene resin containing 10% Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding... |
|||
Izod Impact, Unnotched (ISO) | 20.0 kJ/m² | 9.52 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP FARADEX AS002 ABS (Asia Pacific) LNP* Faradex* AS002 is a compound based on Acrylonitrile Butadiene Styrene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Izod Impact, Unnotched (ISO) | 20.0 - 20.0 kJ/m² @Temperature -30.0 - -30.0 °C |
9.52 - 9.52 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 20.0 kJ/m² Grade Count:1 |
Overview of materials for Polystyrene, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Impact Modified". Each property range of values reported is minimum and maximum values of a.. |
|||
Izod Impact, Unnotched (ISO) | 20.0 - 20.0 kJ/m² @Temperature -30.0 - -30.0 °C |
9.52 - 9.52 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 20.0 kJ/m² Grade Count:1 |
Overview of materials for Polystyrene + Polyphenylene Ether, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene + Polyphenylene Ether, Unreinforced". Each property range of values reported is minimum and .. |
|||
Izod Impact, Unnotched (ISO) | 20.0 kJ/m² @Temperature 23.0 °C |
9.52 ft-lb/in² @Temperature 73.4 °F |
ISO 180/U |
Victrex® PEEK 450CA40 Polyetheretherketone, 40% Carbon Fibre Reinforced Product Description:High performance thermoplastic material, 40% carbon fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, .. |
|||
Izod Impact, Unnotched (ISO) | 20.0 - 45.0 kJ/m² | 9.52 - 21.4 ft-lb/in² | Average value: 26.3 kJ/m² Grade Count:6 |
Overview of materials for Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled". Specific grades with glass content between 35% an.. |
|||
Izod Impact, Unnotched (ISO) | 20.0 - 38.5 kJ/m² | 9.52 - 18.3 ft-lb/in² | Average value: 28.3 kJ/m² Grade Count:3 |
Overview of materials for Polyphenylene Sulfide (PPS), PTFE/Glass-Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), PTFE/Glass-Fiber Filled". Each property range of values reported is minimum.. |
|||
Izod Impact, Unnotched (ISO) | 20.0 - 55.0 kJ/m² | 9.52 - 26.2 ft-lb/in² | Average value: 28.3 kJ/m² Grade Count:11 |
Overview of materials for Nylon 66, Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Bead Filled". Each property range of values reported is minimum and maximum values of ap.. |
|||
Izod Impact, Unnotched (ISO) | 20.0 - 21000 kJ/m² | 9.52 - 9990 ft-lb/in² | Average value: 54.3 kJ/m² Grade Count:46 |
Overview of materials for Nylon 610 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610". Each property range of values reported is minimum and maximum values of appropriate MatWeb e.. |
|||
Izod Impact, Unnotched (ISO) | 20.0 kJ/m² @Temperature -30.0 °C |
9.52 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics NORYL V081 PPE+HIPS (Europe-Africa-Middle East) NORYL V081 is a high flow, UV stabilized PPO/PS blend for TV backplate applications. |
|||
Izod Impact, Unnotched (ISO) | 20.0 kJ/m² @Temperature 23.0 °C |
9.52 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Lubricomp KFL34 Acetal Copolymer (Europe-Africa-Middle East) LNP* Lubricomp* KFL34 is a compound based on Acetal Copolymer resin containing Glass Fiber, PTFE.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Unnotched (ISO) | 20.0 kJ/m² | 9.52 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP OX91041 PPS - LINEAR (Europe-Africa-Middle East) LNP* LUBRICOMP* OX91041 is a compound based on PPS Linear resin containing Carbon Fiber, Glass Fiber, PTFE. Added features include: Internally Lubricated, Electrically Conductive. |
|||
Izod Impact, Unnotched (ISO) | 20.0 kJ/m² | 9.52 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP RFL369 PA6.6 (Europe-Africa-Middle East) LNP* LUBRICOMP* RFL369 is a compound based on PA 66 resin containing Glass Fiber, PTFE, Flame Retardant. Added features include: Flame Retardant, internally lubricated |
|||
Izod Impact, Unnotched (ISO) | 20.0 kJ/m² @Temperature 23.0 °C |
9.52 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Lubricomp WBG16 PBT (Europe-Africa-Middle East) LNP* Lubricomp* WBG16 is a compound based on Polybutylene Terephalate resin containing Glass Bead, Graphite.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Unnotched (ISO) | 20.0 kJ/m² | 9.52 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP ZL003 PPE+PS (Europe-Africa-Middle East) LNP* LUBRICOMP* ZL003 is a compound based on PPE+PS Blend resin containing PTFE. Added features include Internally Lubricated. |
|||
Izod Impact, Unnotched (ISO) | 20.0 kJ/m² | 9.52 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP ZX89743 PPE+PS (Europe-Africa-Middle East) LNP* LUBRICOMP* ZX89743 is a compound based on PPE+PS Blend resin containing Glass Fiber, Glass Beads and a Proprietary Lubricant. Added features include : Internally Lubricated. |
|||
Izod Impact, Unnotched (ISO) | 20.0 kJ/m² | 9.52 ft-lb/in² | ISO 180 |
Solvay Specialty Polymers Ryton® BR111BL Polyphenylene Sulfide (PPS), GlassMineral Filled Ryton® BR111BL Ryton® BR111 is a black-colored glass fiber and mineral filled polyphenylene sulfide compound that provides enhanced mechanical strength with good electrical properties and outs.. |
|||
Izod Impact, Unnotched (ISO) | 20.0 kJ/m² | 9.52 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP STAT-KON DEL329EP PC (Europe-Africa-Middle East) LNP* STATKON* DEL329EP is a compound based on Polycarbonate resin containing Carbon Fiber, PTFE, Flame Retardant. Added features include: Electrically Conductive, Internally Lubricated, Flame retard.. |
|||
Izod Impact, Unnotched (ISO) | 20.0 kJ/m² | 9.52 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics Valox® DR48 PBT (Europe-Africa-Middle East) VALOX DR48 is a 17% glass reinforced, flame retardant injection moulding PBT resin. Applications: lamp sockets, connectors, switches, electrical housings and bases, bobbins, trimmers and electromoto.. |
|||
Izod Impact, Unnotched (ISO) | 20.0 kJ/m² @Temperature -30.0 °C |
9.52 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics Valox® ENH8530 PBT+PET (Europe-Africa-Middle East) Non-Brominated & Non-Chlorinated Flame Retardant, 15% Glass fiber reinforced PBT/PET blend |
|||
Izod Impact, Unnotched (ISO) | 20.0 kJ/m² @Temperature 23.0 °C |
9.52 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Thermocomp MCR13S PP (Europe-Africa-Middle East) LNP* THERMOCOMP* MCR13S is a compound based on Polypropylene resin containing Carbon Fiber, Barium Sulfate. Added features include: Heat Stabilized.This data was supplied by SABIC-IP for the Europe-.. |
|||
Izod Impact, Unnotched (ISO) | 20.0 kJ/m² | 9.52 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP MF006A PP (Europe-Africa-Middle East) LNP* THERMOCOMP* MF006A is a compound based on Polypropylene resin containing Glass Fiber. |
|||
Izod Impact, Unnotched (ISO) | 20.0 kJ/m² @Temperature 23.0 °C |
9.52 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Thermocomp QF002 PA6.10 LNP* Thermocomp* QF002 is a compound based on Nylon 6/10 containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Unnotched (ISO) | 20.0 kJ/m² @Temperature -30.0 °C |
9.52 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics NORYL GFN1V PPE+HIPS (Europe-Africa-Middle East) NORYL GFN1V is a 10 % glass fibre reinforced material with a HDT/A of 110C according ISO 75. NORYL GFN1V cust spec 1977 has been approved for potable water applications up to 85C by the UK WFBS acco.. |
|||
Izod Impact, Unnotched (ISO) | 20.0 kJ/m² | 9.52 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP MF004AS PP LNP THERMOCOMP* MF004AS is a compound based on Polypropylene resin containing 20% Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Izod Impact, Unnotched (ISO) | 20.0 kJ/m² @Temperature 23.0 °C |
9.52 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Thermocomp MFM43S PP (Europe-Africa-Middle East) LNP* THERMOCOMP* MFM43S is a compound based on Polypropylene resin containing Glass Fiber, Mineral. Added features include : Heat Stabilized.This data was supplied by SABIC-IP for the Europe-Africa-.. |
|||
Izod Impact, Unnotched (ISO) | 20.0 kJ/m² | 9.52 ft-lb/in² | ASTM D256 |
Tipco Tipcolite® TMHS 291 Phenolic Compound, Khaki Cotton Fabric, in fluffy form, Soft Flow & High Impact Strength Soft Flow Phenolic Compound, Reinforced with Khakhi Cotton Fabric, in fluffy formApplications: Defence ApplicationsProcessing: Compression MoldingInformation provided by the Manufacturer, Tipco Ind.. |
|||
Izod Impact, Unnotched (ISO) | 20.0 kJ/m² | 9.52 ft-lb/in² | 80x10x4; ISO 180/1U |
Eurostar Starpylen MCR13S PP, 15% Carbon Fiber Filled, Injection Molded Starpylen MCR13S is a 15% Carbon Fiber Reinforced Polypropylene Injection Molding ResinInformation provided by Eurostar. |
|||
Izod Impact, Unnotched (ISO) | 20.0 kJ/m² | 9.52 ft-lb/in² | 80x10x4; ISO 180/1U |
Eurostar Starpylen MH0200A HDPE, Injection Molding Starpylen MH0200A is a High Density Polypropylene Injection Molding ResinInformation provided by Eurostar. |