Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 132 kJ/m² | 62.8 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP AI001XXH ABS LNP* Lubricomp* AI001XXH is a compound based on ABS containing 2% Silicone. Characteristics of this grade are: Healthcare and Internally Lubricated. |