Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 105 kJ/m² @Temperature 23.0 °C |
50.0 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Lubricomp DBL14 PC (Europe-Africa-Middle East) Internally lubricated Polycarbonate compound, comtaining Glass Bead and PTFEThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Unnotched (ISO) | 105 kJ/m² | 50.0 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP DBL32 PC LNP* Lubricomp* DBL32 is a compound based on Polycarbonate resin containing 10% Glass Beads and 15% PTFE. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Unnotched (ISO) | 105 kJ/m² @Temperature 23.0 °C |
50.0 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Thermocomp MX05038 PP (Europe-Africa-Middle East) Polypropylene compound, containing miniral. Added features include High ImpactThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Unnotched (ISO) | 105 kJ/m² | 50.0 ft-lb/in² | ISO 180/1eU |
Lubrizol ESTALOC® T514 Ester-Type, Reinforced Engineering Thermoplastic (European Grade) Description: Estaloc® RETP (Reinforced Engineering Thermoplastic) is a tough, dimensionally stable, abrasion-resistant thermoplastic that withstands demanding environments. Developed as an extensio.. |
|||
Izod Impact, Unnotched (ISO) | 105 kJ/m² | 50.0 ft-lb/in² | 80x10x4; ISO 180/1U |
Eurostar Starpylen MX05038 TPEX, Injection Molded Starpylen MX05038 is a TPEX Injection Molding ResinInformation provided by Eurostar. |
|||
Izod Impact, Unnotched (ISO) | 105 kJ/m² | 50.0 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP DBL32 PC (Asia Pacific) LNP* Lubricomp* DBL32 is a compound based on Polycarbonate resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive, Internally Lubricated. |