Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 100 kJ/m² @Temperature -30.0 °C |
47.6 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1U |
SABIC Innovative Plastics Lexan® 503RS PC (Europe-Africa-Middle East) LEXAN 503RS is a medium viscosity, glass reinforced, flame retardant grade UV stabilized grade. |
|||
Izod Impact, Unnotched (ISO) | 100 kJ/m² | 47.6 ft-lb/in² | 80*10*3; ISO 180/1U |
SABIC Innovative Plastics Lexan® 513RS PC (Europe-Africa-Middle East) LEXAN 513RS is a medium viscosity, glass reinforced, flame retardant grade UV stabilized grade. |
|||
Izod Impact, Unnotched (ISO) | >= 100 kJ/m² | >= 47.6 ft-lb/in² | 80*10*3; ISO 180/1U |
SABIC Innovative Plastics Lexan® ML7686 PC (Europe-Africa-Middle East) Transparent Polycarbonate in limited colors. Excellent processability, super high flow. UL rated V-2 at 1.5mm. |
|||
Izod Impact, Unnotched (ISO) | >= 100 kJ/m² | >= 47.6 ft-lb/in² | 80*10*3; ISO 180/1U |
SABIC Innovative Plastics Lexan® ML7686E PC (Europe-Africa-Middle East) Transparent Polycarbonate in natural color. Excellent processability, super high flow. UL compliant 94V-2 at 1.5mm. |
|||
Izod Impact, Unnotched (ISO) | 100 kJ/m² | 47.6 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP FARADEX MS002 PP LNP* FARADEX* MS002 is a compound based on Polypropylene resin containing 10% Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Izod Impact, Unnotched (ISO) | 100 kJ/m² @Temperature 23.0 °C |
47.6 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Faradex MS002P PP (Europe-Africa-Middle East) LNP* Faradex* MS002P is a compound based on Polypropylene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding, Exceptional Processi.. |
|||
Izod Impact, Unnotched (ISO) | 100 kJ/m² @Temperature 23.0 °C |
47.6 ft-lb/in² @Temperature 73.4 °F |
DAM; ISO 180/1U |
DuPont Performance Polymers Zytel® HTN 53G50HSLR BK083 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTN53G50HSLR BK083 is a 50% glass reinforced, heat stabilized, lubricated high performance polyamide resin developed for moderate temperature structural applications requiring retention of h.. |
|||
Izod Impact, Unnotched (ISO) | >= 100 kJ/m² | >= 47.6 ft-lb/in² | 80*10*3; ISO 180/1U |
SABIC Innovative Plastics Lexan® EXRL1061 PC (Asia Pacific) Transparent Polycarbonate in natural color. Excellent processability, super high flow. |
|||
Izod Impact, Unnotched (ISO) | 100 kJ/m² | 47.6 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP FARADEX MS002 PP (Europe-Africa-Middle East) LNP* Faradex* MS002 is a compound based on Polypropylene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Izod Impact, Unnotched (ISO) | 100 kJ/m² | 47.6 ft-lb/in² | d.a.m.; ISO 180-1U |
Lanxess Durethan® B 30 S FN30 000000 Nylon 6, Flame Retardant PA 6, non-reinforced, injection molding, halogen free flame retardant, heat-aging resistanceInformation provided by LANXESS. |
|||
Izod Impact, Unnotched (ISO) | 100 kJ/m² | 47.6 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP DL003E PC (Asia Pacific) LNP LUBRICOMP* DL003E is a compound based on Polycarbonate resin containing PTFE. Added features of this material include: Easy Molding. |
|||
Izod Impact, Unnotched (ISO) | 100 kJ/m² | 47.6 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP FL004 PE LNP* Lubricomp* FL004 is a compound based on Polyethylene resin containing 20% PTFE. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Unnotched (ISO) | 100 kJ/m² | 47.6 ft-lb/in² | ISO 180/1eU |
Solvay TECHNYLSTARâ„¢ SX 216 V50 PA6, 50% glass filled, Conditioned Description: TECHNYLSTAR Polyamide, reinforced with 50% of glass fiber, characterized by a high fluidity of the melt, for injection molding.Available in: Asia Pacific, Europe and North America Produ.. |
|||
Izod Impact, Unnotched (ISO) | 100 kJ/m² | 47.6 ft-lb/in² | ISO 180/1eU |
Solvay TECHNYLSTARâ„¢ SX 218 L2 V60 Black JA6A PA6, 60% glass filled, Conditioned Description: TECHNYLSTAR polyamide reinforced with 60% of glass fiber, heat and UV stabilized, characterized by a high fluidity of the melt, for injection molding.Available in: Europe Product Applic.. |
|||
Izod Impact, Unnotched (ISO) | 100 kJ/m² | 47.6 ft-lb/in² | ISO 180/1eU |
Solvay TECHNYLSTARâ„¢ SX 218 V50 PA6, 50% glass filled, Conditioned Description: TECHNYLSTARâ„¢ SX 218 V50 is based on a patented high flow polyamide 6 resin (Technylstar), heat stabilized, reinforced with 50% of glass fiber, for injection molding. This product i.. |
|||
Izod Impact, Unnotched (ISO) | 100 kJ/m² @Temperature -40.0 °C |
47.6 ft-lb/in² @Temperature -40.0 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP STAT-KON DX07323 PC+ABS (Asia Pacific) LNP* STAT-KON* DX07323 is a compound based on polycarbonate resin containing conductive fillers. Added features of this compound includes: ESD safe and excellent low-temperature impact performance, .. |
|||
Izod Impact, Unnotched (ISO) | 100 kJ/m² @Temperature -40.0 °C |
47.6 ft-lb/in² @Temperature -40.0 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP STAT-KON DX07323 PC+ABS (Europe-Africa-Middle East) LNP* STAT-KON* DX07323 is a compound based on polycarbonate resin containing conductive fillers. Added features of this compound includes: ESD safe and excellent low-temperature impact performance, .. |
|||
Izod Impact, Unnotched (ISO) | 100 kJ/m² | 47.6 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics Xenoy® X5630Q PC+PET (Europe-Africa-Middle East) Mineral filled PC/PET blend with high heat dimensional stability, low shrinkage and low CTE, especially for painted applications |
|||
Izod Impact, Unnotched (ISO) | 100 kJ/m² | 47.6 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP VERTON RV00AEXP PA 66 (Europe-Africa-Middle East) LNP* VERTON* RV00AEXP is a compound based on PA 66 resin containing Long Glass Fiber. |
|||
Izod Impact, Unnotched (ISO) | 100 kJ/m² | 47.6 ft-lb/in² | DIN 53453 |
Wico Plast Wicotal 500 Acetal ApplicationsInjection moldingAll information provided by Wico Plast, Warenhandelsges. mbH |
|||
Izod Impact, Unnotched (ISO) | 100 kJ/m² | 47.6 ft-lb/in² | 50%RH; ISO 180/1U |
DuPont Performance Polymers Zytel® 8018HS NC010 Nylon 66
(Unverified Data**) 14% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 8018HS NC010 is a 14% glass reinforced heat stabilized toughened polyamide 66 resin.Information provided by DuPont Performance Polym.. |
|||
Izod Impact, Unnotched (ISO) | >= 100 kJ/m² | >= 47.6 ft-lb/in² | 80x10x4; ISO 180/1U |
Eurostar Staramide PX06093 PA6, Impact Modified, Injection Molded Staramide PX06093 is an UV Stabilized, Impact Modified Polyamide 6 Injection Molding Resin (also known as P1000HI020UVL)Information provided by Eurostar. |
|||
Izod Impact, Unnotched (ISO) | 100 - 100 kJ/m² @Temperature -30.0 - -30.0 °C |
47.6 - 47.6 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 100 kJ/m² Grade Count:1 |
Overview of materials for Nylon 6, Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum v.. |
|||
Izod Impact, Unnotched (ISO) | >= 100 kJ/m² @Temperature -30.0 - -30.0 °C |
>= 47.6 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 100 kJ/m² Grade Count:1 |
Overview of materials for Nylon 6, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Extruded". Each property range of values reported is minimum and maximum values of appropriate .. |
|||
Izod Impact, Unnotched (ISO) | 100 kJ/m² | 47.6 ft-lb/in² | DAM; ISO 180/1U |
DuPont Performance Polymers Minlon® 12T BKB100 Nylon 66
(Unverified Data**) 36% Mineral Reinforced Toughened Polyamide 66 Minlon 12T BKB100 is a 36% mineral reinforced toughened heat stabilized black polyamide 66 resin for injection molding.Information provided by DuPont Pe.. |
|||
Izod Impact, Unnotched (ISO) | 100 kJ/m² @Temperature 23.0 °C |
47.6 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Thermotuf PK003EI2 PA 6 (Europe-Africa-Middle East) LNP* THERMOTUF* PK003EI2 is a compound based on PA 6 resin containing Impact Modifier, Mineral. Added features include High Impact, Easy Molding.This data was supplied by SABIC-IP for the Europe-Afr.. |
|||
Izod Impact, Unnotched (ISO) | 100 kJ/m² | 47.6 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP VERTON RV00ASXS PA 66 (Europe-Africa-Middle East) LNP* VERTON* RV00ASXS is a compound based on PA 66 resin containing Long Glass Fiber. Added features include; Heat Stabilized |
|||
Izod Impact, Unnotched (ISO) | 100 kJ/m² @Temperature 23.0 °C |
47.6 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Verton RV00CEU PA 66 (Europe-Africa-Middle East) LNP* VERTON* RV00CEU is a compound based on PA 66 resin containing Long Glass Fiber. Added features include; Easy Molding, UV Stabilized.This data was supplied by SABIC-IP for the Europe-Africa-Midd.. |
|||
Izod Impact, Unnotched (ISO) | 100 kJ/m² @Temperature 23.0 °C |
47.6 ft-lb/in² @Temperature 73.4 °F |
80x10x4mm; ISO 180/1U |
SYNTHOS Krasten® 562E High Impact Polystyrene High impact grade with properties suitable for thermoforming. Processed mainly by extrusion and thermoforming. Production of plates, sheets, technical parts and molded packaging (used in e.g. the fo.. |
|||
Izod Impact, Unnotched (ISO) | 100 kJ/m² | 47.6 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics Xenoy® X5630 PC+PET (Europe-Africa-Middle East) Mineral filled PC/PET blend with high heat dimensional stability, low shrinkage and low CTE, especially for painted applications |