Polymer Property : Adhesive Bond Strength = 284.6 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Adhesive Bond Strength 1.962 MPa

@Temperature 110 °C,
Time 86400 sec
284.6 psi

@Temperature 230 °F,
Time 24.0 hour
Chosun Refractories APM-1 Special Mortar
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Adhesive Bond Strength 1.962 MPa

@Temperature 110 °C,
Time 86400 sec
284.6 psi

@Temperature 230 °F,
Time 24.0 hour
Chosun Refractories ASM_36 Air-Setting Mortar
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Adhesive Bond Strength 1.962 MPa

@Temperature 110 °C,
Time 86400 sec
284.6 psi

@Temperature 230 °F,
Time 24.0 hour
Chosun Refractories ASM-35 Air-Setting Mortar
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Adhesive Bond Strength 1.962 MPa

@Temperature 110 °C,
Time 86400 sec
284.6 psi

@Temperature 230 °F,
Time 24.0 hour
Chosun Refractories ASM-38 Air-Setting Mortar
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Adhesive Bond Strength 1.962 MPa

@Temperature 110 °C,
Time 86400 sec
284.6 psi

@Temperature 230 °F,
Time 24.0 hour
Chosun Refractories ASM-39 Air-Setting Mortar
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Adhesive Bond Strength 1.962 MPa

@Temperature 110 °C,
Time 86400 sec
284.6 psi

@Temperature 230 °F,
Time 24.0 hour
Chosun Refractories ASM-40 Air-Setting Mortar
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Adhesive Bond Strength 1.962 MPa

@Temperature 500 °C,
Time 10800 sec
284.6 psi

@Temperature 932 °F,
Time 3.00 hour
Chosun Refractories BM-2W High-Adhesion Mortar
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Adhesive Bond Strength 1.962 MPa

@Temperature 500 °C,
Time 10800 sec
284.6 psi

@Temperature 932 °F,
Time 3.00 hour
Chosun Refractories BM-3W High-Adhesion Mortar
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Adhesive Bond Strength 1.962 MPa

@Temperature 110 °C,
Time 86400 sec
284.6 psi

@Temperature 230 °F,
Time 24.0 hour
Chosun Refractories GM-1 Special Mortar
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Adhesive Bond Strength 1.962 MPa

@Temperature 110 °C,
Time 86400 sec
284.6 psi

@Temperature 230 °F,
Time 24.0 hour
Chosun Refractories MSM-36 High-Adhesion Mortar
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Adhesive Bond Strength 1.962 MPa

@Temperature 110 °C,
Time 86400 sec
284.6 psi

@Temperature 230 °F,
Time 24.0 hour
Chosun Refractories MSM-38 High-Adhesion Mortar
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Adhesive Bond Strength 1.962 MPa

@Temperature 110 °C,
Time 86400 sec
284.6 psi

@Temperature 230 °F,
Time 24.0 hour
Chosun Refractories MSM-39 High-Adhesion Mortar
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Adhesive Bond Strength 1.962 MPa

@Temperature 110 °C,
Time 86400 sec
284.6 psi

@Temperature 230 °F,
Time 24.0 hour
Chosun Refractories MSM-40 High-Adhesion Mortar
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Adhesive Bond Strength 1.962 MPa

@Temperature 110 °C,
Time 86400 sec
284.6 psi

@Temperature 230 °F,
Time 24.0 hour
Chosun Refractories SCH-2 Special Mortar
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Adhesive Bond Strength 1.962 MPa

@Temperature 110 °C,
Time 86400 sec
284.6 psi

@Temperature 230 °F,
Time 24.0 hour
Chosun Refractories SSM-1 Special Mortar
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Adhesive Bond Strength 1.962 MPa

@Temperature 500 °C,
Time 10800 sec
284.6 psi

@Temperature 932 °F,
Time 3.00 hour
Chosun Refractories SSM-1 Special Mortar
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Adhesive Bond Strength 1.962 MPa

@Temperature 110 °C,
Time 86400 sec
284.6 psi

@Temperature 230 °F,
Time 24.0 hour
Chosun Refractories ZM-2 Special Mortar
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Adhesive Bond Strength 1.962 MPa

@Temperature 110 °C,
Time 86400 sec
284.6 psi

@Temperature 230 °F,
Time 24.0 hour
Chosun Refractories ASM-37 Air-Setting Mortar
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Adhesive Bond Strength 1.962 MPa

@Temperature 110 °C,
Time 86400 sec
284.6 psi

@Temperature 230 °F,
Time 24.0 hour
Chosun Refractories ZM-1 Special Mortar
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).