Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 16.5 MPa @Temperature 177 °C |
2390 psi @Temperature 351 °F |
Lap Shear |
Henkel Hysol PL 737 Film Adhesive Nonmetallic, modified epoxy film specifically designed for use in structural aircraft components. Low flow characteristics.Application: Metal and Honeycomb Bonding |
|||
Adhesive Bond Strength | 16.5 MPa @Temperature 23.9 °C |
2390 psi @Temperature 75.0 °F |
on aluminum; ASTM D1002-64 |
3M Pronto™ CA-7 Instant Adhesive One-part, room-temperature curing adhesive that is ready-to-use without metering or mixing. Bonded parts reach handling strength in 5-10 seconds on many applications.Very fast setting product with .. |