Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Notched Tensile Strength | 2027 - 2192 MPa | 294000 - 317900 psi | |
Latrobe Lescalloy® Jethete M-152 ESR 8" RCS High Strength Stainless Steel LESCALLOY JETHETE M-152 ESR is a nitrogen bearing, hardenable 12% chromium stainless steel intended for various structural components requiring high strength and good oxidation resistance up to 800Â.. |
|||
Notched Tensile Strength | 2027 - 2082 MPa | 294000 - 302000 psi | |
Latrobe Lescalloy® Jethete M-152 ESR 6" RCS High Strength Stainless Steel LESCALLOY JETHETE M-152 ESR is a nitrogen bearing, hardenable 12% chromium stainless steel intended for various structural components requiring high strength and good oxidation resistance up to 800°.. |