| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Charpy Impact Unnotched | 9.20 J/cm² @Temperature 23.0 °C |
43.8 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
| Solvay TECHNYL® C 246SI V30 PA6, 30% glass filled, DRY Description: Polyamide 6, reinforced with 30 % of glass fiber, with high impact resistance, for injection molding.Available in: Asia Pacific , Europe and North AmericaProduct Applications: Having go.. |
|||
| Charpy Impact Unnotched | 9.20 J/cm² @Temperature -30.0 °C |
43.8 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
| Sax Polymers SAXLAC 310A Acrylonitrile Butadiene Styrene Saxalac 310A is a medium viscosity, impact resistant ABS injection molding grade, characterized by good processability and high stiffness.Mechanical property data tested at 50% RH.Information provid.. |
|||
| Charpy Impact Unnotched | 9.20 J/cm² @Temperature 23.0 °C |
43.8 ft-lb/in² @Temperature 73.4 °F |
cond; ISO 179/1eU |
| DSM Novamid® 1010GH30 NAT PA6-GF30 30% Glass Reinforced, Heat Stabilized, Injection Molding |
|||
| Charpy Impact Unnotched | 9.20 J/cm² @Temperature 23.0 °C |
43.8 ft-lb/in² @Temperature 73.4 °F |
cond; ISO 179/1eU |
| DSM Novamid® 1013G30 1 NA PA6-GF30 30% Glass Reinforced, Injection Molding |
|||
| Charpy Impact Unnotched | 9.20 J/cm² @Temperature 23.0 °C |
43.8 ft-lb/in² @Temperature 73.4 °F |
cond; ISO 179/1eU |
| DSM Novamid® 1013GH30 1 NA/BK701 PA6-GF30 30% Glass Reinforced, Heat Stabilized, Injection Molding |
|||
| Charpy Impact Unnotched | 9.20 J/cm² @Temperature 23.0 °C |
43.8 ft-lb/in² @Temperature 73.4 °F |
50%RH; ISO 179/1eU |
| DuPont Performance Polymers Zytel® 70G30HSLR NC010 Nylon 66
(Unverified Data**) Zytel® 70G30HSLR NC010 is a 30% glass fiber reinforced, heat stabilized, hydrolysis resistant polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
| Charpy Impact Unnotched | 9.20 J/cm² @Temperature 23.0 °C |
43.8 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
| Ascend Performance Materials Vydyne® R540 Nylon 66, 40% Glass Reinforced, Conditioned Vydyne® R540 is general-purpose, hydrolysis-resistant, 40% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties when.. |
|||
| Charpy Impact Unnotched | 9.20 J/cm² @Temperature 23.0 °C |
43.8 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
| Ascend Performance Materials Vydyne® R540H Nylon 66, 40% Glass Reinforced, Conditioned Vydyne® R540H is general-purpose, heat-stabilized, hydrolysis-resistant, 40% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of physic.. |
|||
| Charpy Impact Unnotched | 9.20 J/cm² @Temperature 23.0 °C |
43.8 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
| Ascend Performance Materials VYDYNE® R543 Nylon, 43% Glass Reinforced, DAM Vydyne® R543 is general purpose, 43% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine fee, flow and mold release. Glass.. |
|||
| Charpy Impact Unnotched | 9.20 J/cm² @Temperature 23.0 °C |
43.8 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
| Ascend Performance Materials Vydyne® R543H BK02 Nylon 66, 43% Glass Reinforced, DAM Vydyne® R543H BK02 is general-purpose, 43% glass-fiber reinforced PA66 resin. Available in black, it is an injection-molding grade resin that is lubricated for machine feed, flow and mold release. .. |
|||
| Charpy Impact Unnotched | 9.20 J/cm² @Temperature 23.0 °C |
43.8 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
| Ascend Performance Materials Vydyne® R543H Black Nylon 66, 43% Glass Reinforced, DAM Vydyne® R543H Black is general-purpose, hydrolysis-resistant, 43% glass-fiber reinforced PA66 resin. Available in black, it is an injection-molding grade resin that is lubricated for machine feed, .. |
|||
| Charpy Impact Unnotched | 9.20 J/cm² @Temperature 23.0 °C |
43.8 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
| Ascend Performance Materials Vydyne® R543H Natural Nylon 66, 43% Glass Reinforced, DAM Vydyne® R543H Natural is general-purpose, hydrolysis-resistant, 43% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine fe.. |
|||
| Charpy Impact Unnotched | 9.20 J/cm² @Temperature 23.0 °C |
43.8 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
| Ascend Performance Materials Vydyne® R543H NT Nylon 66, 43% Glass Reinforced, DAM Vydyne® R543H NT is general-purpose, 43% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine feed, flow and mold release. .. |
|||
| Charpy Impact Unnotched | 9.20 J/cm² @Temperature 23.0 °C |
43.8 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
| Ascend Performance Materials Vydyne® R543H Nylon 66, 43% Glass Filled, Dry as Molded Vydyne® R543H is general-purpose, 43% glass-reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for improved machine feed, flow and mold release. .. |
|||
| Charpy Impact Unnotched | 9.20 J/cm² @Temperature 23.0 °C |
43.8 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
| Akro-Plastic Akromid® A3 GF 35 (2421) PA 6.6 Dry, 35% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
| Charpy Impact Unnotched | 9.20 J/cm² @Temperature 23.0 °C |
43.8 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
| Ascend Performance Materials Vydyne® R633 Nylon 66 Copolymer, 33% Glass Filled, Conditioned (2.5% Moisture) Vydyne® R633 is 33% glass-fiber reinforced, PA66/6 copolymer resin for superior surface appearance. Available in natural, this injection-molding grade resin is lubricated for machine feed and mold .. |
|||
| Charpy Impact Unnotched | 9.20 J/cm² @Temperature 23.0 °C |
43.8 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
| Ascend Performance Materials Vydyne® R633H Nylon 66/6, 33% Glass Reinforced, Conditioned Vydyne® R633H is 33% glass-fiber reinforced PA66/6 copolymer resin for superior surface appearance. Available in natural, this injection-molding grade resin is lubricated for machine feed and mold .. |
|||
| Charpy Impact Unnotched | 9.20 J/cm² @Temperature 23.0 °C |
43.8 ft-lb/in² @Temperature 73.4 °F |
50%RH; ISO 179/1eU |
| DuPont Performance Polymers Zytel® 70G35HSLX BK357 Nylon 66
(Unverified Data**) Zytel® 70G35HSLX BK357 is a 35% glass fiber reinforced, heat stabilized, black polyamide 66 for injection molding.Information provided by DuPont Performance Polymers |
|||