Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 1.10 - 1.30 J/cm² @Temperature 23.0 °C |
5.24 - 6.19 ft-lb/in² @Temperature 73.4 °F |
Injection; ISO 179/ 1eU |
Raschig Group AMPLA® 7250 melamine-modified polyester Cellulose reinforced melamine-modified Polyester molding compound. Very good electrical values, excellent heat resistance, excellent surface quality, low post shrinkage. This product meets the allow.. |
|||
Charpy Impact Unnotched | 0.800 - 1.30 J/cm² @Temperature 23.0 °C |
3.81 - 6.19 ft-lb/in² @Temperature 73.4 °F |
Injection; ISO 179/ 1eU |
Raschig Group MELOPLAS® 2500 MF Cellulose-reinforced MF molding compound in white and colored shades. Very good electrical properties, high surface hardness, good abrasion- and UV-stability, very good resistance to chemicals - al.. |