Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 20.0 J/cm² @Temperature -30.0 °C |
95.2 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
DuPont Performance Polymers Delrin® FG511DP NC010 Acetal Homopolymer
(Unverified Data**) Delrin® FG511DP is a medium viscosity acetal homopolymer, with improved thermal stability and modifications for more precise molding. It has been developed for consideration into applications such .. |
|||
Charpy Impact Unnotched | 20.0 J/cm² @Temperature -30.0 °C |
95.2 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
DuPont Performance Polymers Delrin® FG900P NC010 Acetal Homopolymer
(Unverified Data**) Delrin® FG900P is a low viscosity acetal homopolymer, with improved thermal stability. It has been developed for consideration into applications such as parts for the food industry.Information prov.. |
|||
Charpy Impact Unnotched | 20.0 J/cm² @Temperature 23.0 °C |
95.2 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
DuPont Performance Polymers Delrin® FG900P NC010 Acetal Homopolymer
(Unverified Data**) Delrin® FG900P is a low viscosity acetal homopolymer, with improved thermal stability. It has been developed for consideration into applications such as parts for the food industry.Information prov.. |
|||
Charpy Impact Unnotched | 20.0 J/cm² @Temperature -30.0 °C |
95.2 ft-lb/in² @Temperature -22.0 °F |
Conditioned; ISO 179/1eU |
Lanxess Durethan® AC 30 000000 Nylon 66 PA 66, injection molding-grade, non-reinforced, higher notched impact strength than A 30 / A 31 in the dry and conditioned stateApplication Examples: plug connectors, cable binders, cable clips, par.. |
|||
Charpy Impact Unnotched | 20.0 J/cm² @Temperature -30.0 °C |
95.2 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
Lanxess Pocan® B 1501 000000 PBT PBT, non-reinforced, injection molding, extrusion, food contact |
|||
Charpy Impact Unnotched | 20.0 J/cm² @Temperature 23.0 °C |
95.2 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Lanxess Pocan® KU 2-7003 000000 PBT PBT, non-reinforced, injection molding |
|||
Charpy Impact Unnotched | 20.0 J/cm² @Temperature -30.0 °C |
95.2 ft-lb/in² @Temperature -22.0 °F |
ISO 179-1eU |
Lanxess Pocan® B 1701 000000 PBT PBT, non-reinforced, extrusion, food contactInformation provided by LANXESS. |
|||
Charpy Impact Unnotched | 20.0 J/cm² @Temperature 23.0 °C |
95.2 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Styrolution Luran® S 757 R Colored ASA Description: General-purpose grade for injection molding with high stiffness.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS |
|||
Charpy Impact Unnotched | 20.0 J/cm² @Temperature -30.0 °C |
95.2 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
BASF Ultraform® E 3120 BM POM Description: Is a POM, high-molecular grade for extrusion blow molding of hollow parts.Information provided by BASF |
|||
Charpy Impact Unnotched | 20.0 J/cm² @Temperature -30.0 °C |
95.2 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
BASF Ultraform® N2320 006 POM Description: Is a POM, high-molecular-weight grade with somewhat increased flowability for injection molding of relatively thick-walled moldings.Information provided by BASF |
|||
Charpy Impact Unnotched | 20.0 J/cm² @Temperature 23.0 °C |
95.2 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
BASF Ultraform® W2320 U035 LEV POM Description: Is a POM, UV-stabilized, very free-flowing, rapidly solidifying grade for injection molding, with reduced emission potential.Information provided by BASF |
|||
Charpy Impact Unnotched | 20.0 J/cm² @Temperature -30.0 °C |
95.2 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
DuPont Performance Polymers Delrin® 511DP NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 511DP is a medium viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage, less shrinkage, fewer voids).Information provided.. |
|||
Charpy Impact Unnotched | 20.0 J/cm² @Temperature 20.0 °C |
95.2 ft-lb/in² @Temperature 68.0 °F |
|
Kennametal Stellite Nucalloy® 430 High-Silicon Nickel-Base Hardfacing Alloy Applications include components of chemical processing.Nucalloy® alloys are unique, patented, high-silicon, nickel-base hardfacing alloys that are designed to have optimum combinations of hardness .. |
|||
Charpy Impact Unnotched | 20.0 J/cm² @Temperature 400 °C |
95.2 ft-lb/in² @Temperature 752 °F |
|
Kennametal Stellite Nucalloy® 430 High-Silicon Nickel-Base Hardfacing Alloy Applications include components of chemical processing.Nucalloy® alloys are unique, patented, high-silicon, nickel-base hardfacing alloys that are designed to have optimum combinations of hardness .. |
|||
Charpy Impact Unnotched | 20.0 J/cm² @Temperature 600 °C |
95.2 ft-lb/in² @Temperature 1110 °F |
|
Kennametal Stellite Nucalloy® 430 High-Silicon Nickel-Base Hardfacing Alloy Applications include components of chemical processing.Nucalloy® alloys are unique, patented, high-silicon, nickel-base hardfacing alloys that are designed to have optimum combinations of hardness .. |
|||
Charpy Impact Unnotched | 20.0 J/cm² @Temperature -30.0 °C |
95.2 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
Lanxess Pocan® B 1600 000000 PBT PBT, non-reinforced, injection molding, extrusion, food contact |