Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 2.00 J/cm² @Temperature -20.0 °C |
9.52 ft-lb/in² @Temperature -4.00 °F |
STN EN ISO 179 |
Plastcom SLOVALEN PC 51 C 40 Polypropylene Homopolymer and Copolymer, 40% Micronized Talc FeaturesModified homopolymer and copolymer PP for injection moulding with the content of 40% micronized, chemically modified talc. Increased strength, rigidity and thermal application up to 120°C... |
|||
Charpy Impact Unnotched | 2.00 J/cm² @Temperature 23.0 °C |
9.52 ft-lb/in² @Temperature 73.4 °F |
STN EN ISO 179 |
Plastcom SLOVALEN PC 59 GF 13 Compounded Polypropylene Homopolymer, 13% Chemically Coupled Glass Fiber FeaturesCompounded homopolymer PP, with the content of 13% chemically coupled glass fiber and modifier of mechanical properties. Increased strength in comparison with unfilled PP. Use in all indus.. |
|||
Charpy Impact Unnotched | 2.00 J/cm² @Temperature 23.0 °C |
9.52 ft-lb/in² @Temperature 73.4 °F |
|
Plastcom SLOVALEN PC 71 GF 10 PP, 10% glass fibre FeaturesCompouded homopolymer PP, with the content of 10% chemically bound glass fibre and modifier of mechanical properties. Increased strength in comparison with unfilled PP. Use in all industry s.. |
|||
Charpy Impact Unnotched | 2.00 J/cm² @Temperature -20.0 °C |
9.52 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVALEN PC 71 T 10 PP, 10% mineral filling FeaturesModified copolymer PP for injection moulding with the content of 10% mineral filling. Increased rigidity, strength and thermal use up to 130°C depending on the talc content. Decr eased shri.. |
|||
Charpy Impact Unnotched | 2.00 J/cm² @Temperature -20.0 °C |
9.52 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVAMID 6 GF 10 FRC 2 PA6, 10% glass fibre, flame retardant FeaturesPA 6 for injection moulding, chemically strengthened with 10 % glass fibre. Application: impacted mouldings and mouldings with high strength applied in automotive, electrical, engineering an.. |
|||
Charpy Impact Unnotched | 2.00 J/cm² @Temperature -20.0 °C |
9.52 ft-lb/in² @Temperature -4.00 °F |
STN EN ISO 179 |
Plastcom SLOVAMID 6 GF 15 LS Polyamide 6, 15% Glass Fiber, UV Stabilization FeaturesPA 6 for injection moulding, chemically reinforced with 15% glass fiber, stabilized against UV-radiation. Used for the grips of electric tools, hobby tools, gears, covers of electric tools... |
|||
Charpy Impact Unnotched | 2.00 J/cm² @Temperature -20.0 °C |
9.52 ft-lb/in² @Temperature -4.00 °F |
STN EN ISO 179 |
Plastcom SLOVAMID 6 GF 15 T 25 Polyamide 6, 15% Glass Fiber, 25% Micronized Talc FeaturesGood anisotropy of the manufacturing shrinkage. The talc is added to get the material shrinkage identical in both directions. Application for flat products in disc form / no screw after co.. |
|||
Charpy Impact Unnotched | 2.00 J/cm² @Temperature -20.0 °C |
9.52 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVAMID 6 GF 5 T 20 FRG 2 PA6, 5% glass fibre, 20% mineral filling FeaturesPA 6 for injection moulding, with halogen free flame retardant based on polyphosphate. Good anisotrophi shinking. Application for the electrical industry: protectors, coil forms, covers, ter.. |
|||
Charpy Impact Unnotched | 2.00 J/cm² @Temperature 23.0 °C |
9.52 ft-lb/in² @Temperature 73.4 °F |
STN EN ISO 179 |
Plastcom SLOVAMID 66 GF 10 GB 20 Polyamide 66, 10% Glass Fiber, 20% Glass Beads FeaturesPA 66 chemically reinforced with 10% glass fiber and with the content of 20% glass beads. Improved anisotropy of shrinkage. The relation of the anisotropy to the mechanical properties can .. |
|||
Charpy Impact Unnotched | 2.00 J/cm² @Temperature 23.0 °C |
9.52 ft-lb/in² @Temperature 73.4 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics Cycoloy® C4210 PC+ABS (Europe-Africa-Middle East) CYCOLOY C4210 is a 10% glass reinforced, non-FR PC+ABS grade. It shows high heat resistance, excellent strength and rigidity with good cosmetic appearance. It combines a good processabity with a low.. |
|||
Charpy Impact Unnotched | 2.00 J/cm² @Temperature -40.0 °C |
9.52 ft-lb/in² @Temperature -40.0 °F |
DIN 53453 |
LATI LARIL 13 G/20 20% Glass Fiber Reinforced Polyphenylene Oxide (PPOm)
(Unverified Data**) Description: Laril thermoplastics are polyphenylene oxide (PPOm) products. They exhibit excellent toughness, even at low temperatures, good thermal resistance and dimensional stability are the most .. |
|||
Charpy Impact Unnotched | 2.00 J/cm² @Temperature -20.0 °C |
9.52 ft-lb/in² @Temperature -4.00 °F |
DIN 53453 |
LATI LARIL 13 G/20-V1 20% Glass Fiber Reinforced Polyphenylene Oxide (PPOm) (UL94V-1)
(Unverified Data**) Description: Laril thermoplastics are polyphenylene oxide (PPOm) products. They exhibit excellent toughness, even at low temperatures, good thermal resistance and dimensional stability are the most .. |
|||
Charpy Impact Unnotched | 2.00 J/cm² @Temperature 23.0 °C |
9.52 ft-lb/in² @Temperature 73.4 °F |
DAM; ISO 179/1eU |
DuPont Performance Polymers Zytel® FR70M30V0 BK010 Nylon 66
(Unverified Data**) Zytel® FR70M30V0 BK010 is a 30% mineral reinforced, flame retardant, black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Charpy Impact Unnotched | 2.00 J/cm² @Temperature -30.0 °C |
9.52 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
Lanxess Durethan® DP 1100/30 H2.0 901510 Nylon 6, Micro Glass Balls PA6, molding grade, micro glass balls, good heat-ageing resistance |
|||
Charpy Impact Unnotched | 2.00 J/cm² @Temperature 23.0 °C |
9.52 ft-lb/in² @Temperature 73.4 °F |
|
LATI Larton GCE/600 PPS, Glass/Mineral Reinforced Polyphenylene Sulfide (PPS) based compound. Glass fibers / Mineral filler. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa .. |
|||
Charpy Impact Unnotched | 2.00 J/cm² @Temperature -20.0 °C |
9.52 ft-lb/in² @Temperature -4.00 °F |
|
LATI Larton GCE/600 PPS, Glass/Mineral Reinforced Polyphenylene Sulfide (PPS) based compound. Glass fibers / Mineral filler. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa .. |
|||
Charpy Impact Unnotched | 2.00 J/cm² @Temperature 0.000 °C |
9.52 ft-lb/in² @Temperature 32.0 °F |
ISO 179/1eU |
Inno-Comp INNOPOL® CS 1-2120 AP 20% Talc Filled Polypropylene Homopolymer INNOPOL CS 1-2120 AP is a 20 % talc filled compound based on polypropylene homopolymer. This grade is available in natural and custom colored form.INNOPOL® CS 1-2120 AP is recommended especially.. |
|||
Charpy Impact Unnotched | 2.00 J/cm² @Temperature 23.0 °C |
9.52 ft-lb/in² @Temperature 73.4 °F |
|
LATI Laramid G/15 PPA, 15% Glass Fiber Reinforced Semi-aromatic polyamide (PPA) based compound. Glass fibers. Very good thermal properties. Good chemical resistance. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; .. |
|||
Charpy Impact Unnotched | 2.00 J/cm² @Temperature 23.0 °C |
9.52 ft-lb/in² @Temperature 73.4 °F |
|
LATI Latamid 66 S/30 PA 66, 30% Glass Bead Reinforced Polyamide 66 (PA66) based compound. Glass beads. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p.A. |
|||
Charpy Impact Unnotched | 2.00 J/cm² @Temperature 23.0 °C |
9.52 ft-lb/in² @Temperature 73.4 °F |
|
LATI Latene® AG7H2 G/50 PP Homopolymer, 50% Glass Fiber Reinforced, Heat Stabilized Polypropylene homopolymer (PPh) based compound. Chemical grafting Heat stabilized. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation prov.. |
|||
Charpy Impact Unnotched | 2.00 J/cm² @Temperature -30.0 °C |
9.52 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics Ultem 2412EPR PEI 40% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.This data was supplied by SABIC-IP for the Am.. |
|||
Charpy Impact Unnotched | 2.00 J/cm² @Temperature 23.0 °C |
9.52 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Styrolution Luran® HH-120 Alpha-Methylstyrene Acrylonitrile Luran HH-120 is a grade of AMSAN with high heat resistance and improved mechanical strength. It is suitable for injection molding and extrusion applications and can be used as a modifier for high he.. |
|||
Charpy Impact Unnotched | 2.00 J/cm² @Temperature -20.0 °C |
9.52 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eU |
Borealis HB601WG Polypropylene Homopolymer HB601WG is a polypropylene homopolymer intended for injection molding and blow molding. The product is available in natural but other colors can be provided on request. This material has excellent .. |
|||
Charpy Impact Unnotched | 2.00 J/cm² @Temperature -20.0 °C |
9.52 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVALEN PH 21 T 20 PP, 20% mineral filling FeaturesModified homopolymer PP for injection moulding with the content of 20% mineral filling. Increased rigidity, strength and thermal use up to 130°C depending on the talc content. Decreased shr.. |
|||
Charpy Impact Unnotched | 2.00 J/cm² @Temperature -40.0 °C |
9.52 ft-lb/in² @Temperature -40.0 °F |
DIN 53453 |
LATI LASTIROL TR G/10-V1 10% Glass Fiber Reinforced Polystyrene (PS) (UL94 V-1)
(discontinued **) Description: Lastirol thermoplastics are polystyrene (PS) products. The Lastirols feature excellent dimensional stability, good flowability, and can be molded without any particular problem. Glass f.. |
|||
Charpy Impact Unnotched | 2.00 J/cm² @Temperature -20.0 °C |
9.52 ft-lb/in² @Temperature -4.00 °F |
|
LATI Kelon® A FR H2 CETG/300-V0 PA 66, Glass/Mineral Reinforced, Flame Retardant, Heat Stabilized Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers / Mineral filler. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. Low thermal expansion .. |
|||
Charpy Impact Unnotched | 2.00 J/cm² @Temperature -20.0 °C |
9.52 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVALEN PC 92 T 40 PP, 40% mineral filling FeaturesModified homopolymer and copolymer PP for injection moulding with the contenct of 40% microground, chemically modified talc. Increased strength, rigidity and thermal application up to 100°C.. |
|||
Charpy Impact Unnotched | 2.00 J/cm² @Temperature 23.0 °C |
9.52 ft-lb/in² @Temperature 73.4 °F |
DIN 53453 |
LATI LARTON G/40 40% Glass Fiber Filled Polyphenylene sulfide (PPS)
(Unverified Data**) Description: Larton thermoplastics are polyphenylene sulfide (PPS) products. They are distinguished by a group of very interesting properties combined with easy moldability. Larton parts feature: ex.. |
|||
Charpy Impact Unnotched | 2.00 J/cm² @Temperature -30.0 °C |
9.52 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
Sax Polymers SAXALEN PPH329B20 Polypropylene Homopolymer, 20% Glass Filled SAXALEN PPH329B20 is a 20% glass beads filled Polypropylene - Homopolymer intended for injection molding. Low shrinkage, low warpage gradeInformation provided by SAX Polymers |