Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 15.0 J/cm² @Temperature -20.0 °C |
71.4 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVASTER® B1 BT PBT, basic type FeaturesPBT basic type for injection molding. Melt is characterised by outstanding fluidity, which enables injection molding of complicated and divided products also on multiple molds. Anisotropy of.. |
|||
Charpy Impact Unnotched | 15.0 J/cm² @Temperature -20.0 °C |
71.4 ft-lb/in² @Temperature -4.00 °F |
DIN 53453 |
LATI LASTANE 50 G/25 25% Glass Fiber Reinforced Polyurethane (PUR)
(Unverified Data**) Description: Lastane thermoplastics are polyurethane (PUR) products. They exhibit good wear and impact resistance, even at low temperatures, noise inertness and excellent mould release. These proper.. |
|||
Charpy Impact Unnotched | >= 15.0 J/cm² @Temperature 23.0 °C |
>= 71.4 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1eU |
Ineos ABS Triax® KU2-3154 ABS + Polyamide Blend (Conditioned), Injection Molding Grade Triax® KU2-3154 is mineral reinforced, easy-flowing, injection molding grade, and comes in pellets. It has reduced moisture absorption and very low warpage. |
|||
Charpy Impact Unnotched | 15.0 J/cm² @Temperature -30.0 °C |
71.4 ft-lb/in² @Temperature -22.0 °F |
Conditioned; ISO 179/1eU |
Lanxess Durethan® A 30 S 000000 Nylon 66 PA 66 standard injection molding-grade, non-reinforced, good demolding, very rapid solidificationApplication Examples: plug connectors, terminal blocks, cable clips, bobbins |
|||
Charpy Impact Unnotched | 15.0 J/cm² @Temperature 23.0 °C |
71.4 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Lanxess Durethan® A 30 S 000000 Nylon 66 PA 66 standard injection molding-grade, non-reinforced, good demolding, very rapid solidificationApplication Examples: plug connectors, terminal blocks, cable clips, bobbins |
|||
Charpy Impact Unnotched | 15.0 J/cm² @Temperature 23.0 °C |
71.4 ft-lb/in² @Temperature 73.4 °F |
d.a.m.; ISO 179-1eU |
Lanxess Durethan® A 30 S H3.0 000000 Nylon 66, Injection Molding PA 66, non-reinforced, injection moldingInformation provided by LANXESS. |
|||
Charpy Impact Unnotched | 15.0 J/cm² @Temperature 23.0 °C |
71.4 ft-lb/in² @Temperature 73.4 °F |
d.a.m.; ISO 179-1eU |
Lanxess Durethan® B 30 S F30 000000 Nylon 6, Flame Retardant PA 6, non-reinforced, injection molding, flame retardantInformation provided by LANXESS. |
|||
Charpy Impact Unnotched | >= 15.0 J/cm² @Temperature 23.0 °C |
>= 71.4 ft-lb/in² @Temperature 73.4 °F |
Conditioned; ISO 179/1eU |
Lanxess Durethan® DP 1100/30 H2.0 901510 Nylon 6, Micro Glass Balls PA6, molding grade, micro glass balls, good heat-ageing resistance |
|||
Charpy Impact Unnotched | 15.0 J/cm² @Temperature -30.0 °C |
71.4 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
Lanxess Pocan® B 1300 000000 PBT PBT, non-reinforced, injection molding, extrusion |
|||
Charpy Impact Unnotched | 15.0 J/cm² @Temperature -30.0 °C |
71.4 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
Lanxess Pocan® B 1305 000000 PBT PBT, non-reinforced, injection molding |
|||
Charpy Impact Unnotched | 15.0 J/cm² @Temperature -30.0 °C |
71.4 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
Lanxess Pocan® KU 1-7301 000000 PBT PBT, non-reinforced, injection molding, food contact |
|||
Charpy Impact Unnotched | 15.0 J/cm² @Temperature 23.0 °C |
71.4 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1eU |
Ineos ABS Lustran® ABS E211 LNS013 Pellets (a-methylstyrene-SAN-modified), Extrusion Grade Lustran® ABS E211 LNS013 is extrusion grade with high heat resistance. It is used for the production of molded plastic articles. |
|||
Charpy Impact Unnotched | 15.0 J/cm² @Temperature -30.0 °C |
71.4 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
Styrolution Luran® S 776 S Colored ASA Description: Injection molding grade with good toughness and strength. Uses include parts for garden equipment, parts for office chairs and antennas.Information provided by STYROLUTION, which is a j.. |
|||
Charpy Impact Unnotched | 15.0 J/cm² @Temperature -30.0 °C |
71.4 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
Styrolution Luran® S 776 S UV ASA Description: Injection molding grade with good toughness and strength. Uses include parts for garden equipment, parts for office chairs and antennas.Information provided by STYROLUTION, which is a j.. |
|||
Charpy Impact Unnotched | 15.0 J/cm² @Temperature -30.0 °C |
71.4 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
Styrolution Luran® S 796 M Colored ASA Description: High-impact injection molding gr4ade with good flowability.Applications: Trim panels for goods vehicles.Information provided by STYROLUTION, which is a joint venture between BASF and IN.. |
|||
Charpy Impact Unnotched | 15.0 J/cm² @Temperature 23.0 °C |
71.4 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Styrolution Novodur® E211 ABS Novodur E211 is a high heat extrusion grade and suitable for blow moldingInformation provided by Styrolution |
|||
Charpy Impact Unnotched | <= 15.0 J/cm² @Temperature 23.0 °C |
<= 71.4 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Styrolution Polystyrol 454 C GR 2 PS Description: Polystyrol 454 C is an impact resistant polystyrene with a good balance of toughness, high flow, heat resistance and high gloss.Applications: TV-front panels and back covers, VCR fronts.. |
|||
Charpy Impact Unnotched | 15.0 J/cm² @Temperature 23.0 °C |
71.4 ft-lb/in² @Temperature 73.4 °F |
80x10x4mm; ISO 179/1eU |
SYNTHOS Krasten® 662E High Impact Polystyrene High impact grade with properties suitable for thermoforming. Processed mainly by extrusion and thermoforming. Production of demanding visual appearance plates, technical parts, sheets and molded pa.. |
|||
Charpy Impact Unnotched | 15.0 J/cm² @Temperature 23.0 °C |
71.4 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Styrolution Terblend® N 3154 ASA / PA, 8% Mineral filled Terblend N 3154 is an 8% mineral filled ABS/PA blend with good dimensional stability and enhanced rigidity.High dimensional stabilityEnhanced rigidityMineral filled (8%)Information provided by Styro.. |
|||
Charpy Impact Unnotched | 15.0 J/cm² @Temperature 23.0 °C |
71.4 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Borealis Daplen™ EG103AI Polypropylene Compound, Mineral Filled Daplen™ EG103AI is a 15 % mineral filled polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness and high melt flow rate.. |
|||
Charpy Impact Unnotched | 15.0 J/cm² @Temperature -30.0 °C |
71.4 ft-lb/in² @Temperature -22.0 °F |
longitudinal; ISO 179/1eU |
Bond Laminates TEPEX® dynalite 201-C200(x)/45% Carbon – PA6.6 Consolidated Composite Laminate Within the TEPEX® composite laminate, Polyamide 66 is a resin known for its high hardness, stiffness, abrasion resistance, heat and chemical resistances. The carbon used within this material is ae.. |
|||
Charpy Impact Unnotched | 15.0 J/cm² @Temperature -30.0 °C |
71.4 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
BASF Ultraform® N2770 K POM Description: Is a POM, injection-molding grade with improved wear characteristics for sliding elements.Information provided by BASF |
|||
Charpy Impact Unnotched | 15.0 J/cm² @Temperature 23.0 °C |
71.4 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
BASF Ultraform® N2770 K POM Description: Is a POM, injection-molding grade with improved wear characteristics for sliding elements.Information provided by BASF |
|||
Charpy Impact Unnotched | 15.0 J/cm² @Temperature -30.0 °C |
71.4 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
BASF Ultraform® W2320 003 PRO POM Description: Is a POM, is a very easy flowing grade for thin-walled components with long flow paths.Information provided by BASF |
|||
Charpy Impact Unnotched | 15.0 J/cm² @Temperature 23.0 °C |
71.4 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
BASF Ultraform® W2320 003 PRO POM Description: Is a POM, is a very easy flowing grade for thin-walled components with long flow paths.Information provided by BASF |
|||
Charpy Impact Unnotched | 15.0 J/cm² @Temperature -30.0 °C |
71.4 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
BASF Ultraform® W2320 U03 POM Description: Very free-flowing, rapidly solidifying grade with UV stabilization for use where processing is extremely difficult but mechanical requirements are lower.Information provided by BASF |
|||
Charpy Impact Unnotched | 15.0 J/cm² @Temperature -30.0 °C |
71.4 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
DuPont Performance Polymers Delrin® 911DP NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 911DP is a low viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage, less shrinkage, fewer voids).Information provided by.. |
|||
Charpy Impact Unnotched | 15.0 J/cm² @Temperature 23.0 °C |
71.4 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1eU |
Ineos ABS Triax® KU2-3154 ABS + Polyamide Blend (DAM), Injection Molding Grade Triax® KU2-3154 is mineral reinforced, easy-flowing, injection molding grade, and comes in pellets. It has reduced moisture absorption and very low warpage. |