Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 9.30 J/cm² @Temperature -20.0 °C |
44.3 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVAMID 66 MI LS PA66, improved strength FeaturesModified with thermoplastic reactive caoutchouc, determined for mouldings with high toughness also at minus temperatures. Eligible application for ski-shoes, helmets for sport and other safe.. |
|||
Charpy Impact Unnotched | 9.30 J/cm² @Temperature 23.0 °C |
44.3 ft-lb/in² @Temperature 73.4 °F |
50%RH; ISO 179/1eU |
DuPont Performance Polymers Zytel® 70G30L NC010 Nylon 66
(Unverified Data**) Zytel® 70G30L NC010 is a 30% glass fiber reinforced polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Charpy Impact Unnotched | 9.30 J/cm² @Temperature 23.0 °C |
44.3 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Sax Polymers SAXAMID 136F6Q32 Nylon 6, 30% Glass Fiber SAXAMID 136F6Q32 is a high-impact-modified polyamide 6 injection-molding-grade reinforced with 30% glass fibers . Beside the high impact strength at low temperatures this grade shows very good proce.. |
|||
Charpy Impact Unnotched | 9.30 J/cm² @Temperature 23.0 °C |
44.3 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Sax Polymers SAXAMID 226F8 Nylon 6.6, 40% Glass Fiber SAXAMID 226F8 is a general purpose polyamide 6.6 injection-molding-grade reinforced with 40% glass fibers. It has very high mechanical strength.Information provided by SAX Polymers |
|||
Charpy Impact Unnotched | 9.30 J/cm² @Temperature 23.0 °C |
44.3 ft-lb/in² @Temperature 73.4 °F |
cond; ISO 179/1eU |
DSM Akulon® K222-KGV4 /A PA6-GF20 FR(30) 20% Glass Reinforced, Heat Stabilized, Flame Retardant (Halogen-phosphorous-free) |
|||
Charpy Impact Unnotched | 9.30 J/cm² @Temperature 23.0 °C |
44.3 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
BASF Ultramid® HMG14 HS BK 102 60% Glass Filled PA66 (Conditioned) Description: Ultramid HMG14 HS BK-102 is a 60% glass reinforced, injection molding grade of PA66 offering high strength and stiffness. Due to inherently lower moisture absorption, Ultramid HMG14 HS .. |