Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 8.40 J/cm² @Temperature -30.0 °C |
40.0 ft-lb/in² @Temperature -22.0 °F |
50%RH; ISO 179/1eU |
DuPont Performance Polymers Zytel® 73G30HSL NC010 Nylon 6
(Unverified Data**) Zytel® 73G30HSL NC010 is a 30% glass fiber reinforced, heat stabilized polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Charpy Impact Unnotched | 8.40 J/cm² @Temperature 23.0 °C |
40.0 ft-lb/in² @Temperature 73.4 °F |
Conditioned; ISO 179/1eU |
Lanxess Durethan® DP 1801/30 H3.0 000000 Nylon 6, 30% Milled Glass Fiber PA 6, injection molding grade, 30% milled fibers, UL 94V-2 at 0.8 mm, max. temperature in glow wire test: 960 °C at 0,75 mm, "halogen-free", good heat-ageing resistanceApplication Examples: Medic.. |
|||
Charpy Impact Unnotched | 8.40 J/cm² @Temperature -30.0 °C |
40.0 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
Sax Polymers SAXAMID 226F8 Nylon 6.6, 40% Glass Fiber SAXAMID 226F8 is a general purpose polyamide 6.6 injection-molding-grade reinforced with 40% glass fibers. It has very high mechanical strength.Information provided by SAX Polymers |
|||
Charpy Impact Unnotched | 8.40 J/cm² @Temperature -30.0 °C |
40.0 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
Suzhou Hipro Polymers Hiprolon® 400 MC HLS G30 Nylon, 30% glass fiber filled Hiprolon® 400 MC HLS G30 is a specialty long chain polyamide compound reinforced with 30% chopped glass fiber for injection molding. It contains some bio-renewable resources Features: high dime.. |
|||
Charpy Impact Unnotched | 8.40 J/cm² @Temperature 23.0 °C |
40.0 ft-lb/in² @Temperature 73.4 °F |
cond; ISO 179/1eU |
DSM Novamid® 3021GH30 NAT PA66-GF30 30% Glass Reinforced, Heat Stabilized |
|||
Charpy Impact Unnotched | 8.40 J/cm² @Temperature 23.0 °C |
40.0 ft-lb/in² @Temperature 73.4 °F |
cond; ISO 179/1eU |
DSM Novamid® 3021GH30 BK629 PA66-GF30 30% Glass Reinforced, Heat Stabilized |
|||
Charpy Impact Unnotched | 8.40 J/cm² @Temperature 23.0 °C |
40.0 ft-lb/in² @Temperature 73.4 °F |
DAM; ISO 179/1eU |
DuPont Performance Polymers Zytel® 70G35HSRX BK099 Nylon 66
(Unverified Data**) Zytel® 70G35HSRX BK099 a 35% glass reinforced, heat stabilized, hydrolysis resistant PA66 for injection molding. Developed for applications designed for direct overmolding of gaskets onto thermopla.. |