Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 0.600 J/cm² @Temperature -20.0 °C |
2.86 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVALEN PH 61 B 70 PP, 70% mineral filling FeaturesModified PP for injection moulding with the content of 70% of barium sulphate. Increased density. Decreased shrinkage.Used for production of vertical blind weights. Delivered in natural mode.. |
|||
Charpy Impact Unnotched | 0.600 - 0.800 J/cm² @Temperature 23.0 °C |
2.86 - 3.81 ft-lb/in² @Temperature 73.4 °F |
Compression; ISO 179/ 1eU |
Raschig Group AMPLA® 2000 melamine-modified polyester Halogen-free, organically and inorganically filled melamine-modified Polyester molding compound. Low post-shrinkage, very good electrical values, high heat resistance, very good sliding behavior, ve.. |
|||
Charpy Impact Unnotched | 0.600 - 0.800 J/cm² @Temperature 23.0 °C |
2.86 - 3.81 ft-lb/in² @Temperature 73.4 °F |
Compression; ISO 179/ 1eU |
Raschig Group AMPLA® 2500 melamine-modified polyester Halogen-free, organically and inorganically filled melamine-modified Polyester molding compound. Excellent elasticity and shock resistance, low post-shrinkage, very good electrical values, high heat.. |
|||
Charpy Impact Unnotched | 0.600 - 0.900 J/cm² @Temperature 23.0 °C |
2.86 - 4.28 ft-lb/in² @Temperature 73.4 °F |
Compression; ISO 179/ 1eU |
Raschig Group MELOPLAS® 152.7 MF Cellulose-reinforced MF molding compound in white and colored shades. High surface hardness, very good UV stability, very good resistance to chemicals also to foodstuff ingredients, physiologically.. |
|||
Charpy Impact Unnotched | 0.600 - 0.900 J/cm² @Temperature 23.0 °C |
2.86 - 4.28 ft-lb/in² @Temperature 73.4 °F |
Compression; ISO 179/ 1eU |
Raschig Group MELOPLAS® 181.5 MF Cellulose-reinforced, phenol-modified MF molding compound (MPF) in white and colored shades. Very good electrical properties, high surface hardness, good mechanical strength, high UV and heat resis.. |
|||
Charpy Impact Unnotched | 0.600 J/cm² @Temperature -30.0 °C |
2.86 ft-lb/in² @Temperature -22.0 °F |
DAM; ISO 179/1eU |
DuPont Performance Polymers Minlon® EFE6096 GY090A Nylon 66
(Unverified Data**) Minlon® EFE6096 GY090A is a 15% mineral reinforced impact modified nylon 66 resin.Information provided by DuPont Performance Polymers |
|||
Charpy Impact Unnotched | 0.600 - 0.900 J/cm² @Temperature 23.0 °C |
2.86 - 4.28 ft-lb/in² @Temperature 73.4 °F |
Injection; ISO 179/ 1eU |
Raschig Group MELOPLAS® 180 MF Wood flour-reinforced, phenol-modified MF molding compound (MPF) in dark colors. High surface hardness, good mechanical strength and electrical properties, good heat resistance. Self-extinguishing .. |