Mechanical Properties Metric English Comments
Charpy Impact Unnotched 3.40 J/cm²

@Temperature -20.0 °C
16.2 ft-lb/in²

@Temperature -4.00 °F
Plastcom SLOVALEN PH 99 GB 30 LS PP, 30% glass beads, mod. of mech. properties
FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 30% glass beads, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP...
Charpy Impact Unnotched 3.40 J/cm²

@Temperature -30.0 °C
16.2 ft-lb/in²

@Temperature -22.0 °F
ISO 179
PolyOne OnFlex™ BIO 5180D-E0014 Thermoplastic Elastomer (TPE)
OnFlex™ BIO 5100 series thermoplastic elastomer compounds are glass reinforced thermoplastic polyurethane compounds made from renewable natural sources. These compounds contain at least 20% renewab..
Charpy Impact Unnotched 3.40 J/cm²

@Temperature 23.0 °C
16.2 ft-lb/in²

@Temperature 73.4 °F
DIN 53453
Qualchem Danamid FGFLX2-30 Polyamide 6, 30% Glass Fiber
Reinforced with glass fiber. Flame retardant, halogen-free (V-2)Information provided by Qualchem Zrt.
Charpy Impact Unnotched 3.40 J/cm²

@Temperature 23.0 °C
16.2 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Sax Polymers SAXAMID 126K6 Nylon 6, 30% Glass Filled
SAXAMID 126K6 is a 30% glass beads filled polyamide 6 injection-molding-grade. It is characterized by dimensional stability, low warpage and good surface quality.Information provided by SAX Polymers..
Charpy Impact Unnotched 3.40 J/cm²

@Temperature 23.0 °C
16.2 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Sax Polymers SAXAMID 226K6 Nylon 6.6, 30% Glass Beads
SAXAMID 226K6 is a polyamide 6.6 injection-molding-grade filled with 30% glass beads. It is characterized by optimized shrinkage properties.Information provided by SAX Polymers
Charpy Impact Unnotched 3.40 J/cm²

@Temperature -30.0 °C
16.2 ft-lb/in²

@Temperature -22.0 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eU
SABIC Innovative Plastics Valox® VX4015 PBT (Europe-Africa-Middle East)
VALOX VX4015 is a 15% glass reinforced PBT injection moulding resin, with excellent hydrolytical stability.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Charpy Impact Unnotched 3.40 J/cm²

@Temperature 23.0 °C
16.2 ft-lb/in²

@Temperature 73.4 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eU
SABIC Innovative Plastics Valox® VX5530 PBT (Europe-Africa-Middle East)
VALOX VX5530 is a flame retarded, 15% glass fibre reinforced, 10% mineral filled PBT+PC blend with excellent low warpage characteristics.This data was supplied by SABIC-IP for the Europe-Africa-Midd..
Charpy Impact Unnotched 3.40 J/cm²

@Temperature -30.0 °C
16.2 ft-lb/in²

@Temperature -22.0 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eU
SABIC Innovative Plastics Valox® VX5530 PBT (Europe-Africa-Middle East)
VALOX VX5530 is a flame retarded, 15% glass fibre reinforced, 10% mineral filled PBT+PC blend with excellent low warpage characteristics.This data was supplied by SABIC-IP for the Europe-Africa-Midd..
Copyright © lookpolymers.com All Rights Reserved