Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 0.500 - 0.900 J/cm² @Temperature 23.0 °C |
2.38 - 4.28 ft-lb/in² @Temperature 73.4 °F |
Compression; ISO 179/ 1eU |
Raschig Group MELOPLAS® 152 MF Cellulose-reinforced MF molding compound in white and colored shades. Very good electrical properties, high surface hardness, good abrasion- and UV-stability, very good resistance to chemicals - al.. |
|||
Charpy Impact Unnotched | 0.600 - 0.900 J/cm² @Temperature 23.0 °C |
2.86 - 4.28 ft-lb/in² @Temperature 73.4 °F |
Compression; ISO 179/ 1eU |
Raschig Group MELOPLAS® 152.7 MF Cellulose-reinforced MF molding compound in white and colored shades. High surface hardness, very good UV stability, very good resistance to chemicals also to foodstuff ingredients, physiologically.. |
|||
Charpy Impact Unnotched | 0.500 - 0.900 J/cm² @Temperature 23.0 °C |
2.38 - 4.28 ft-lb/in² @Temperature 73.4 °F |
Compression; ISO 179/ 1eU |
Raschig Group MELOPLAS® 181 MF Cellulose-reinforced, phenol-modified MF molding compound (MPF) in white and colored shades. High surface hardness, good electrical properties, good mechanical strength, high UV and heat resistanc.. |
|||
Charpy Impact Unnotched | 0.600 - 0.900 J/cm² @Temperature 23.0 °C |
2.86 - 4.28 ft-lb/in² @Temperature 73.4 °F |
Compression; ISO 179/ 1eU |
Raschig Group MELOPLAS® 181.5 MF Cellulose-reinforced, phenol-modified MF molding compound (MPF) in white and colored shades. Very good electrical properties, high surface hardness, good mechanical strength, high UV and heat resis.. |
|||
Charpy Impact Unnotched | 0.700 - 0.900 J/cm² @Temperature 23.0 °C |
3.33 - 4.28 ft-lb/in² @Temperature 73.4 °F |
Compression; ISO 179/ 1eU |
Raschig Group MELOPLAS® 3025 MF Cellulose-reinforced and inorganically filled MF molding compound in white and colored shades. High surface hardness, good UV and heat stability, very good resistance to chemicals - also to foodstu.. |
|||
Charpy Impact Unnotched | 0.600 - 0.900 J/cm² @Temperature 23.0 °C |
2.86 - 4.28 ft-lb/in² @Temperature 73.4 °F |
Injection; ISO 179/ 1eU |
Raschig Group MELOPLAS® 180 MF Wood flour-reinforced, phenol-modified MF molding compound (MPF) in dark colors. High surface hardness, good mechanical strength and electrical properties, good heat resistance. Self-extinguishing .. |