Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 5.20 J/cm² @Temperature -20.0 °C |
24.7 ft-lb/in² @Temperature -4.00 °F |
STN EN ISO 179 |
Plastcom SLOVALEN PH 49 GF 30 Polypropylene Homopolymer, 30% Glass Fiber FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 30% glass fiber, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP.. |
|||
Charpy Impact Unnotched | 5.20 J/cm² @Temperature -20.0 °C |
24.7 ft-lb/in² @Temperature -4.00 °F |
STN EN ISO 179 |
Plastcom SLOVALEN PH 49 GF 50 Polypropylene Homopolymer, 50% Glass Fiber FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 50% glass fiber, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP.. |
|||
Charpy Impact Unnotched | 5.20 J/cm² @Temperature -20.0 °C |
24.7 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Polykemi AB POLYfill PP CIQ15020 Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||
Charpy Impact Unnotched | 5.20 J/cm² @Temperature 23.0 °C |
24.7 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Polykemi AB SCANBLEND P AP2060 F20 PBT/ASA, Glass Fiber Reinforced Information provided by Polykemi AB |
|||
Charpy Impact Unnotched | 5.20 J/cm² @Temperature -30.0 °C |
24.7 ft-lb/in² @Temperature -22.0 °F |
|
Radici Radiflam® A RV250AF (cond.) Nylon 66-25GF Radiflam® A is a range of flame retardant polyamides 66 (PA 66) used for injection molding and extrusion for all applications where high fire resistance is required.Information provided by Radici g.. |
|||
Charpy Impact Unnotched | 5.20 J/cm² @Temperature 23.0 °C |
24.7 ft-lb/in² @Temperature 73.4 °F |
|
Radici Radilon® S RCV3515 (dry) Nylon 6 Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group. |
|||
Charpy Impact Unnotched | 5.20 J/cm² @Temperature 23.0 °C |
24.7 ft-lb/in² @Temperature 73.4 °F |
|
Plastcom SLOVALEN PC 69 GF 40 PP, 40% glass beads, mod. of mech. properties FeaturesModified copolymer PP for injection moulding, chemically reinforced with 40% glass fibre, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP. A.. |
|||
Charpy Impact Unnotched | 5.20 J/cm² @Temperature -20.0 °C |
24.7 ft-lb/in² @Temperature -4.00 °F |
STN EN ISO 179 |
Plastcom SLOVALEN PH 49 GF 30 003/3M Polypropylene reinforced with glass fiber, heat stabilized Modified homopolymer PP for injection molding, reinforced with 30% glass fiber, heat stabilized. Delivered in black color.Information Provided by Plastcom spol. s r.o. |
|||
Charpy Impact Unnotched | 5.20 J/cm² @Temperature -20.0 °C |
24.7 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVALEN PH 49 GF 30 LW PP, 30% glass fibre, coupling agents, laser writer FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 30% glass fibre, contains the modifier of mechanical properties and contains modificator for laser labeling of fini.. |
|||
Charpy Impact Unnotched | 5.20 J/cm² @Temperature 23.0 °C |
24.7 ft-lb/in² @Temperature 73.4 °F |
|
Radici Radilon® S RCP3010LK (cond.) Nylon 6 PA6 30% Glass Fiber and mineral filler reinforced injection molding grade. Good stiffness and good dimensional stability. Heat stabilized, good surface finish.Information provided by Radici group. |
|||
Charpy Impact Unnotched | 5.20 J/cm² @Temperature -30.0 °C |
24.7 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
Sax Polymers SAXATEC 4307 Acrylonitrile Styrene Acrylate SAXATEC 4307 is a high impact resistant, high viscosity and weatherable ASA injection molding grade, characterized by high mechanical strength and good processabilityInformation provided by SAX Poly.. |
|||
Charpy Impact Unnotched | 5.20 J/cm² @Temperature 23.0 °C |
24.7 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Borealis ME266U Polypropylene Compound, Mineral Filled ME266U is a 20% mineral filled polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness and gives a good surface quality. .. |
|||
Charpy Impact Unnotched | 5.20 J/cm² @Temperature 23.0 °C |
24.7 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Akro-Plastic Akromid® B3 GF 15 (2469) PA 6 Dry, 15% Glass Filled AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Charpy Impact Unnotched | 5.20 J/cm² @Temperature 23.0 °C |
24.7 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
BASF Ultradur® B 4040 G10 50% Glass Filled BK 15029 PBT + PET Description: Injection molding grade with 50% glass fibers for industrial parts with excellent surface quality, for example external door handles in vehicles, visible sunroof frames, oven door handl.. |
|||
Charpy Impact Unnotched | 5.20 J/cm² @Temperature 23.0 °C |
24.7 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
DuPont Performance Polymers Rynite® 530 BK503 PET
(Unverified Data**) Rynite® 530 BK503 is a 30% glass reinforced modified polyethylene terephthalate with outstanding balance of strength, stiffness, and toughness, excellent electrical properties, surface appearance, .. |