Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 4.50 J/cm² @Temperature -20.0 °C |
21.4 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVALEN EH 96 FRD 2 PP, flame retardant FeaturesDetermined for environment, where contact with water is possible, because the electric properties do not change by conditioning. Application - terminals, coil forms, guides in washing machin.. |
|||
Charpy Impact Unnotched | 4.50 J/cm² @Temperature 23.0 °C |
21.4 ft-lb/in² @Temperature 73.4 °F |
STN EN ISO 179 |
Plastcom SLOVALEN PC 51 C 30 Polypropylene Homopolymer and Copolymer, 30% Micronized Talc FeaturesModified homopolymer and copolymer PP for injection moulding with the content of 30% micronized, chemically modified talc. Increased strength, rigidity and thermal application up to 120°C... |
|||
Charpy Impact Unnotched | 4.50 J/cm² @Temperature -20.0 °C |
21.4 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVALEN PH 49 GF 40 PP, 40% glass fibre PP homopolymer for injection moulding, chemically strengthened with 40% of glass fibre, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-go.. |
|||
Charpy Impact Unnotched | 4.50 J/cm² @Temperature -20.0 °C |
21.4 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVAMID 6 GF 10 FRA 5 PA6, 10% glass fibre, flame retardant FeaturesPA 6 for injection moulding, chemically reinforced with 10% glass fibre, with halogen flame retardant. Main features: flammability in accordance with UL 94 V0 at 1.6 mm, glow wire at 960°C,.. |
|||
Charpy Impact Unnotched | 4.50 J/cm² @Temperature 23.0 °C |
21.4 ft-lb/in² @Temperature 73.4 °F |
|
Plastcom SLOVAMID 6 GF 20 PA6, 20% glass beads FeaturesNearly ideal anisotropy of shrinkage in the vertical and in the horizontal direction is established. Manufacturing of exact mouldings. Disadvantage are the relatively low mechanical properti.. |
|||
Charpy Impact Unnotched | 4.50 J/cm² @Temperature -20.0 °C |
21.4 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVAMID 66 GF 25 FRI 3 TS PA66, 25% glass fibre, flame retardant FeaturesPA 66 for injection moulding, chemically reinforced with 25% glass fibre and non-halogen flame retardant, with heat resistance and nonflammability, achieves V 0 in accordance with UL 94. Non.. |
|||
Charpy Impact Unnotched | 4.50 J/cm² @Temperature -20.0 °C |
21.4 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Polykemi AB POLYfill PP CQX10030E10 F Polypropylene, Mineral Reinforced, Elastomer Modified Information provided by Polykemi AB |
|||
Charpy Impact Unnotched | 4.50 J/cm² @Temperature -20.0 °C |
21.4 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Polykemi AB POLYfill PP CQX8025 R2 Polypropylene, Mineral Reinforced, Scratch Resistant Information provided by Polykemi AB |
|||
Charpy Impact Unnotched | 4.50 J/cm² @Temperature 23.0 °C |
21.4 ft-lb/in² @Temperature 73.4 °F |
STN EN ISO 179 |
Plastcom SLOVAMID 6 GF 20 Polyamide 6, 20% Glass Fiber FeaturesPA 6 for injection moulding, chemically coupled with 20% glass fiber. Application: impacted mouldings and mouldings with high strength applied in automotive, electrical, engineering and con.. |
|||
Charpy Impact Unnotched | 4.50 J/cm² @Temperature 23.0 °C |
21.4 ft-lb/in² @Temperature 73.4 °F |
DAM; ISO 179/1eU |
DuPont Performance Polymers Zytel® 105F BK010 Nylon 66
(Unverified Data**) Zytel® 105F BK010 is a lubricated, fast cycling, weather resistant PA 66 resin. Zytel® 105F BK010 contains finely dispersed carbon black.Information provided by DuPont Performance Polymers |
|||
Charpy Impact Unnotched | 4.50 J/cm² @Temperature 23.0 °C |
21.4 ft-lb/in² @Temperature 73.4 °F |
conditioned; ISO 179-1eU |
Lanxess Durethan® AKV 15 FN 00 000000 Nylon 66, 12% Glass Fiber PA 66, 12% glass fiber, injection molding, halogen free flame retardantInformation provided by LANXESS. |
|||
Charpy Impact Unnotched | 4.50 J/cm² @Temperature -30.0 °C |
21.4 ft-lb/in² @Temperature -22.0 °F |
Conditioned; ISO 179/1eU |
Lanxess Durethan® BG 30 X 000000 Nylon 6, 30% Glass Fiber PA 6, injection molding grade, 30% glass fibers/glass spheres, good surface, low warpage |
|||
Charpy Impact Unnotched | 4.50 J/cm² @Temperature 23.0 °C |
21.4 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Lanxess Durethan® BKV 20 FN00 000000 Nylon 6, 18% Glass Fiber PA6, injection molding grade, 18% glass fibers, UL94 V-0 at 0,75 mm ( in house test), free of halogen and red phosphorus, specially for electro/electronic applications in regard to IEC60335-1 |
|||
Charpy Impact Unnotched | 4.50 J/cm² @Temperature 23.0 °C |
21.4 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Lanxess Pocan® B 3215 Z 000000 PBT, 10% Glass Fiber PBT, 10% glass fibers, injection molding, impact modified |
|||
Charpy Impact Unnotched | 4.50 J/cm² @Temperature 23.0 °C |
21.4 ft-lb/in² @Temperature 73.4 °F |
|
LATI Larpeek 10 G/15 PEEK, 15% Glass Fiber Reinforced Polyetheretherketone (PEEK) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Charpy Impact Unnotched | 4.50 J/cm² @Temperature 23.0 °C |
21.4 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Sax Polymers SAXAMID 226F3 Nylon 6.6, 15% Glass Fiber SAXAMID 226F3 is a polyamide 6.6 injection-molding-grade reinforced with 15% glass fibers. This grade is suitable for applications requiring high strength and very good flow properties during proces.. |
|||
Charpy Impact Unnotched | 4.50 J/cm² @Temperature 23.0 °C |
21.4 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Borealis PS65T20 Polypropylene Compound, Mineral Filled PS65T20 is a 20% mineral filled polypropylene compound intended for injection and back injection molding. This material has excellent balanced mechanical properties and high melt flow rate. Applic.. |
|||
Charpy Impact Unnotched | 4.50 J/cm² @Temperature 23.0 °C |
21.4 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
DSM Akulon® K222-KWGV4 Nylon 6-20% Glass Reinforced (European and Asian Grade) (Cond) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Charpy Impact Unnotched | 4.50 J/cm² @Temperature -30.0 °C |
21.4 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
DSM Akulon® K224-G3 (Dry) 15% Glass Reinforced Nylon 6 (North America) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Charpy Impact Unnotched | 4.50 J/cm² @Temperature -30.0 °C |
21.4 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
DSM Akulon® K224-HG3 Nylon 6-15% Glass Reinforced (European and Asian Grade) (Cond) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Charpy Impact Unnotched | 4.50 J/cm² @Temperature 23.0 °C |
21.4 ft-lb/in² @Temperature 73.4 °F |
dry; ISO 179/1eU |
DSM Novamid® 1010GN7-20 BK37 PA6-GF20 FR(30) 0 20% Glass Reinforced, Flame Retardant, Halogen free |
|||
Charpy Impact Unnotched | 4.50 J/cm² @Temperature 23.0 °C |
21.4 ft-lb/in² @Temperature 73.4 °F |
ISO 179/eU |
Eurotec® Tecomid® NA40 GR15 NL PA 6.6 15% glass fiber reinforced Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Charpy Impact Unnotched | 4.50 J/cm² @Temperature 23.0 °C |
21.4 ft-lb/in² @Temperature 73.4 °F |
ISO 179/eU |
Eurotec® Tecomid® NA40 GR15 NL XA 20 PA 6.6 15% glass fiber reinforced, UL94 V0 Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Charpy Impact Unnotched | 4.50 J/cm² @Temperature 23.0 °C |
21.4 ft-lb/in² @Temperature 73.4 °F |
ISO 179/eU |
Eurotec® Tecomid® NA40 NL XA 20 PA 6.6 unreinforced, UL94 V0 Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Charpy Impact Unnotched | 4.50 J/cm² @Temperature 23.0 °C |
21.4 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1eU |
Barlog Plastics KEBATER BF110 PBT, 10% glass fiber reinforced PBT-GF10Information provided by BARLOG plastics GmbH. |
|||
Charpy Impact Unnotched | 4.50 J/cm² @Temperature -30.0 °C |
21.4 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
Akro-Plastic Akromid® T6 GF30 (3501) PPA Dry, 30% Glass Filled The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high.. |
|||
Charpy Impact Unnotched | 4.50 J/cm² @Temperature -30.0 °C |
21.4 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
DSM Arnite® TV4 241 SL PBT-GF20 FR(17) 20% Glass Reinforced, Flame Retardant, UV Stabilized |
|||
Charpy Impact Unnotched | 4.50 J/cm² @Temperature -30.0 °C |
21.4 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
DSM Arnite® TV4 261 KL PBT-GF30 30% Glass Reinforced, Light Stabilized |
|||
Charpy Impact Unnotched | 4.50 J/cm² @Temperature 23.0 °C |
21.4 ft-lb/in² @Temperature 73.4 °F |
STN EN ISO 179 |
Plastcom SLOVAMID 6 T 30 Polyamide 6, 30% Micronized Talc FeaturesDecreased shrinkage against the BT types, increased heat application up to 170°C. Increased tensile modulus - strength of the material. PA matrix reduction. Application for tools, fillin.. |
|||
Charpy Impact Unnotched | 4.50 J/cm² @Temperature -30.0 °C |
21.4 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
DuPont Performance Polymers Sorona® 3030GV NC010 Polytrimethylene Terephthalate (PTT)
(Unverified Data**) Sorona® 3030GV NC010 is a 30% glass reinforced PTT resin containing 25% renewably sourced ingredients by weight (37% based on polymer only) with low warpage and superior strength, stiffness and sur.. |