Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 1.90 J/cm² @Temperature 23.0 °C |
9.04 ft-lb/in² @Temperature 73.4 °F |
DIN 53453 |
Qualchem Danamid FEWLX2-25 Polyamide 6, 25% Mineral Filled Filled with minerals. Flame retardant, halogen-free (V-2)Information provided by Qualchem Zrt. |
|||
Charpy Impact Unnotched | 1.90 J/cm² @Temperature -30.0 °C |
9.04 ft-lb/in² @Temperature -22.0 °F |
DIN 53453 |
Qualchem Danamid FEWLX2-25 Polyamide 6, 25% Mineral Filled Filled with minerals. Flame retardant, halogen-free (V-2)Information provided by Qualchem Zrt. |
|||
Charpy Impact Unnotched | 1.90 J/cm² @Temperature -30.0 °C |
9.04 ft-lb/in² @Temperature -22.0 °F |
|
Radici Radiflam® S RV250FR (cond.) Nylon 6 Radiflam® S is a range of flame retardant polyamides 6 (PA 6) used for injection molding and extrusion for all applications where high fire resistance is required.Information provided by Radici gro.. |
|||
Charpy Impact Unnotched | 1.90 J/cm² @Temperature -30.0 °C |
9.04 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
Sax Polymers SAXALEN PPH335T20 Polypropylene Homopolymer, 20% Talc Filled SAXALEN PPH335T20 is a 20% mineral filled Polypropylene - Homopolymer intended for injection molding with very good flow properties and higher stiffness by low warpage and good surface appearance.In.. |
|||
Charpy Impact Unnotched | 1.90 J/cm² @Temperature -20.0 °C |
9.04 ft-lb/in² @Temperature -4.00 °F |
DIN 53453 |
LATI LARIL 13 G/30-V1 30% Glass Fiber Reinforced Polyphenylene Oxide (PPOm) (UL94V-1)
(Unverified Data**) Description: Laril thermoplastics are polyphenylene oxide (PPOm) products. They exhibit excellent toughness, even at low temperatures, good thermal resistance and dimensional stability are the most .. |
|||
Charpy Impact Unnotched | 1.90 J/cm² @Temperature -40.0 °C |
9.04 ft-lb/in² @Temperature -40.0 °F |
DIN 53453 |
LATI LARIL 13 G/30-V1 30% Glass Fiber Reinforced Polyphenylene Oxide (PPOm) (UL94V-1)
(Unverified Data**) Description: Laril thermoplastics are polyphenylene oxide (PPOm) products. They exhibit excellent toughness, even at low temperatures, good thermal resistance and dimensional stability are the most .. |