Mechanical Properties Metric English Comments
Charpy Impact Unnotched 0.600 J/cm²

@Temperature -20.0 °C
2.86 ft-lb/in²

@Temperature -4.00 °F
Plastcom SLOVALEN PH 61 B 70 PP, 70% mineral filling
FeaturesModified PP for injection moulding with the content of 70% of barium sulphate. Increased density. Decreased shrinkage.Used for production of vertical blind weights. Delivered in natural mode..
Charpy Impact Unnotched 0.600 - 0.800 J/cm²

@Temperature 23.0 °C
2.86 - 3.81 ft-lb/in²

@Temperature 73.4 °F
Compression; ISO 179/ 1eU
Raschig Group AMPLA® 2000 melamine-modified polyester
Halogen-free, organically and inorganically filled melamine-modified Polyester molding compound. Low post-shrinkage, very good electrical values, high heat resistance, very good sliding behavior, ve..
Charpy Impact Unnotched 0.600 - 0.800 J/cm²

@Temperature 23.0 °C
2.86 - 3.81 ft-lb/in²

@Temperature 73.4 °F
Compression; ISO 179/ 1eU
Raschig Group AMPLA® 2500 melamine-modified polyester
Halogen-free, organically and inorganically filled melamine-modified Polyester molding compound. Excellent elasticity and shock resistance, low post-shrinkage, very good electrical values, high heat..
Charpy Impact Unnotched 0.600 - 0.900 J/cm²

@Temperature 23.0 °C
2.86 - 4.28 ft-lb/in²

@Temperature 73.4 °F
Compression; ISO 179/ 1eU
Raschig Group MELOPLAS® 152.7 MF
Cellulose-reinforced MF molding compound in white and colored shades. High surface hardness, very good UV stability, very good resistance to chemicals also to foodstuff ingredients, physiologically..
Charpy Impact Unnotched 0.600 - 0.900 J/cm²

@Temperature 23.0 °C
2.86 - 4.28 ft-lb/in²

@Temperature 73.4 °F
Compression; ISO 179/ 1eU
Raschig Group MELOPLAS® 181.5 MF
Cellulose-reinforced, phenol-modified MF molding compound (MPF) in white and colored shades. Very good electrical properties, high surface hardness, good mechanical strength, high UV and heat resis..
Charpy Impact Unnotched 0.600 J/cm²

@Temperature -30.0 °C
2.86 ft-lb/in²

@Temperature -22.0 °F
DAM; ISO 179/1eU
DuPont Performance Polymers Minlon® EFE6096 GY090A Nylon 66  (Unverified Data**)
Minlon® EFE6096 GY090A is a 15% mineral reinforced impact modified nylon 66 resin.Information provided by DuPont Performance Polymers
Charpy Impact Unnotched 0.600 - 0.900 J/cm²

@Temperature 23.0 °C
2.86 - 4.28 ft-lb/in²

@Temperature 73.4 °F
Injection; ISO 179/ 1eU
Raschig Group MELOPLAS® 180 MF
Wood flour-reinforced, phenol-modified MF molding compound (MPF) in dark colors. High surface hardness, good mechanical strength and electrical properties, good heat resistance. Self-extinguishing ..