Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 44.0 MPa | 6380 psi | |
Lehmann & Voss LUVOCOM® 80-0837-1 Polyacetal-copolymer, with PTFE, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl.. |
|||
Tensile Stress | 44.0 MPa | 6380 psi | At break; ISO 527 |
FKuR Kunststoff Biograde® C 6530 Biodegradable Plastic Compound BIOGRADE® are easy to process blends based on cellulose. BIOGRADE® is composed mainly of natural resources. Based on cellulose, a product of the paper industry BIOGRADE® has been especial.. |
|||
Tensile Stress | 44.0 MPa | 6380 psi | |
Lehmann & Voss LUVOCOM® AC-80/TF/22/BK Polyacetal-copolymer, with PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl.. |
|||
Tensile Stress | 44.0 MPa @Strain 1.00 %, Time 3.60e+6 sec |
6380 psi @Strain 1.00 %, Time 1000 hour |
DIN 53444 |
Wolf Kunststoff ZEDEX® ZX-324VMT A3B PEEK, Fiber Reinforced Main Characteristics: Maximum rigidity; Very good wear resistance; Low stick-slip tendency; Stress resistantApplications: Shipbuilding; Chemical Engineering; Automitve Technology; Machine ToolsInfor.. |
|||
Tensile Stress | 44.0 MPa @Strain 1.00 %, Time 3.60e+6 sec |
6380 psi @Strain 1.00 %, Time 1000 hour |
DIN 53444 |
Wolf Kunststoff ZEDEX® ZX-750V5KF 055 Polymer Alloy. Fiber Reinforced Main Characteristics: Stiff; High elongation and yield stress; Low thermal expansion; Impact resistantApplications: Textile Machinery; Compressors; Hinges; Handling; Machine Tools; Automitve Technol.. |