Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 0.345 MPa @Strain 300 % |
50.0 psi @Strain 300 % |
ASTM D412 |
Teknor Apex Monprene® MP 1231D Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Stress | 0.345 MPa @Strain 300 % |
50.0 psi @Strain 300 % |
ASTM D412 |
Teknor Apex Monprene® MP-1672A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Stress | 0.345 MPa @Strain 300 % |
50.0 psi @Strain 300 % |
ASTM D412 |
Teknor Apex Monprene® MP-1900 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Stress | 0.345 MPa @Strain 300 % |
50.0 psi @Strain 300 % |
ASTM D412 |
Teknor Apex Monprene® MP-1900-R Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |