Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 2.60 MPa @Strain 100 %, Temperature 23.0 °C |
377 psi @Strain 100 %, Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Versaflex™ OM 2262 Thermoplastic Elastomer (TPE) Versaflex™ OM 2262 is a performance overmolding grade with general FDA compliance. This product is designed for both insert and two-shot molding onto Eastman Tritan™ copolyester as well as ABS, PC.. |
|||
Tensile Stress | 2.60 MPa @Strain 100 % |
377 psi @Strain 100 % |
Across Flow; ASTM D412 |
ExxonMobil Santoprene® 121-70B230 Thermoplastic Elastomer A soft, black thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material is specially formulated to bond to sulfur or peroxide-cured thermoset EPDM rubber for corner .. |
|||
Tensile Stress | 2.60 MPa @Strain 100 % |
377 psi @Strain 100 % |
Across Flow; ASTM D412 and ISO 37 |
ExxonMobil Santoprene® 121-70M350 Thermoplastic Vulcanizate - UV Resistant Product Description: A soft, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material is designed for gap filler applications requiring scratch.. |
|||
Tensile Stress | 2.60 MPa @Strain 100 % |
377 psi @Strain 100 % |
Across Flow; ASTM D412 |
ExxonMobil Santoprene® 171-64 Thermoplastic Elastomer A soft, black, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as those.. |
|||
Tensile Stress | 2.60 MPa @Strain 100 % |
377 psi @Strain 100 % |
Across Flow; ASTM D412 |
ExxonMobil Santoprene® 201-64 Thermoplastic Elastomer A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra.. |
|||
Tensile Stress | 2.60 MPa @Strain 100 % |
377 psi @Strain 100 % |
Across Flow; ASTM D412 |
ExxonMobil Santoprene® 271-64 Thermoplastic Elastomer A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as t.. |
|||
Tensile Stress | 2.60 MPa @Strain 100 % |
377 psi @Strain 100 % |
Across Flow; ASTM D412 |
ExxonMobil Santoprene® 241-64 Thermoplastic Elastomer A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with NSF 61 for plumbing applications in contact with potable water and NSF 51 f.. |
|||
Tensile Stress | 2.60 MPa @Strain 100 % |
377 psi @Strain 100 % |
Across Flow; ASTM D412 |
ExxonMobil Santoprene® 101-64 Thermoplastic Elastomer Product Description: A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for.. |