Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 105 MPa | 15200 psi | |
Lehmann & Voss LUVOCOM® 1105-8451 PEEK, with carbon fiber, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.High dimensionally stable precisio.. |
|||
Tensile Stress | 105 MPa | 15200 psi | |
Lehmann & Voss LUVOCOM® 1105-8534 PEEK, with mineral filler Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Reduced moment of inertia compared with metal parts.Chemical and hydrolysis resistance par.. |
|||
Tensile Stress | 105 MPa | 15200 psi | |
Lehmann & Voss LUVOCOM® 1106-8124 Polyether imide, lubricant modified Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le.. |
|||
Tensile Stress | 105 MPa | 15200 psi | |
Lehmann & Voss LUVOCOM® 1301-7648/BK PPS, linear, with glass fiber Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Strong, stiff parts.High continuous use and heat distortion temperature. Non flammable.High chemic.. |
|||
Tensile Stress | 105 MPa | 15200 psi | |
Lehmann & Voss LUVOCOM® 1301-8306 PPS, linear, with carbon fiber, lubricant modified Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Strong, stiff parts.Improved friction and wear behaviour. Emergency running property.Inherent flam.. |
|||
Tensile Stress | 105 MPa | 15200 psi | |
Lehmann & Voss LUVOCOM® 1-8491 Polyamide 66, with carbon fiber, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.High dimensionally stab.. |
|||
Tensile Stress | 105 MPa | 15200 psi | |
Lehmann & Voss LUVOCOM® 1850-7952 PBT, with glass fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec.. |
|||
Tensile Stress | 105 MPa | 15200 psi | |
Lehmann & Voss LUVOCOM® 1850-8023 PBT, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricit.. |
|||
Tensile Stress | 105 MPa | 15200 psi | |
Lehmann & Voss LUVOCOM® 50/CF/15/TF/15/SI/2/BK Polycarbonate, with carbon fiber, PTFE, lubricant modified Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi.. |
|||
Tensile Stress | 105 MPa | 15200 psi | |
Lehmann & Voss LUVOCOM® 50/CF/15/TF/15/SI/2/BK-HB Polycarbonate, with carbon fiber, PTFE, lubricant modified Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi.. |
|||
Tensile Stress | 105 MPa | 15200 psi | |
Lehmann & Voss LUVOCOM® 50-7110 Polycarbonate, with carbon fiber, low-warpage, easy flowing Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Electrically conductive, suitable for continuous discharging o.. |
|||
Tensile Stress | 105 MPa | 15200 psi | |
Lehmann & Voss LUVOCOM® 50-7154/V0 Polycarbonate, with carbon fiber, low-warpage Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Strong, stiff parts.Reduced moment of inertia compared with me.. |
|||
Tensile Stress | 105 MPa | 15200 psi | |
Lehmann & Voss LUVOCOM® 50-7446 Polycarbonate, with carbon fiber, PTFE, lubricant modified Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi.. |
|||
Tensile Stress | 105 MPa | 15200 psi | |
Lehmann & Voss LUVOCOM® 55-7880 PC/ABS Alloy, with carbon fiber and glass fiber Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Strong, stiff parts.Reduced moment of inertia compared with me.. |
|||
Tensile Stress | 105 MPa | 15200 psi | |
Lehmann & Voss LUVOCOM® 1105-7107 PEEK, with glass fiber, easy flowing Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.High dimensionally stable precisio.. |