Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 70.0 MPa | 10200 psi | |
Akro-Plastic Akromid® A28 1 S3 PA, Dry-Impact Resistant
(discontinued **) The product types are mainly used in the automobile industry sector, but also for the domestic industry, the building industry and the leisure time-and sporting goods industry, AKROMID has become a .. |
|||
Tensile Stress | 70.0 MPa | 10200 psi | |
Lehmann & Voss LUVOCOM® 1301-8349 PPS, linear, with PTFE Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Improved friction and wear behaviour. Emergency running property.Low warpage, isotropic shrinkage .. |
|||
Tensile Stress | 70.0 MPa | 10200 psi | |
Lehmann & Voss LUVOCOM® 1301-8386 PPS, linear, with aramid reinforcement and PTFE Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Improved friction and wear behaviour. Emergency running property.Low warpage.dynamic stressInforma.. |
|||
Tensile Stress | 70.0 MPa | 10200 psi | |
Lehmann & Voss LUVOCOM® 1850-7431 PBT, with carbon fiber and glass spheres Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Low warpage.Low waterabsorbtion, for dimensional stable precision parts.Par.. |
|||
Tensile Stress | 70.0 MPa | 10200 psi | |
Lehmann & Voss LUVOCOM® 19-7330 Polyamide 46, with PTFE, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Reduced moment of inertia compared with metal parts.Highly dimensionally stable at elevated tem.. |
|||
Tensile Stress | 70.0 MPa | 10200 psi | |
Lehmann & Voss LUVOCOM® 19-7810 Polyamide 46, with aramid reinforcement and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Good friction and wear behaviour especially at increased temperatures.Emergency running propert.. |
|||
Tensile Stress | 70.0 MPa | 10200 psi | |
Lehmann & Voss LUVOCOM® 50/GF/10/TF/18/SI/2/GY5 Polycarbonate, with glass fiber, PTFE, lubricant modified Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi.. |
|||
Tensile Stress | 70.0 MPa | 10200 psi | |
Lehmann & Voss LUVOCOM® 50-0828 Polycarbonate, with glass fiber, PTFE, lubricant modified Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi.. |
|||
Tensile Stress | 70.0 MPa | 10200 psi | |
Lehmann & Voss LUVOCOM® 50-7164/BL02 Polycarbonate, with glass fiber and PTFE Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Reduced moment of inertia compared with metal parts.Low warpag.. |
|||
Tensile Stress | 70.0 MPa | 10200 psi | |
Lehmann & Voss LUVOCOM® 80/CF/10/BK Polyacetal-copolymer, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Electrically conductive, suitable for continuous discharging of statically .. |
|||
Tensile Stress | 70.0 MPa | 10200 psi | |
Lehmann & Voss LUVOCOM® 80-7653 Polyacetal-copolymer, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Antistatic.No change of electric potential at bearings in case of separation of charge caused b.. |
|||
Tensile Stress | 70.0 MPa | 10200 psi | |
Lehmann & Voss LUVOCOM® 1105/GR/15/TF/15-2 PEEK, with PTFE, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Dynamic stressed parts at high movement velocity.Chemical and hydrolysis resistance parts,.. |
|||
Tensile Stress | 70.0 MPa | 10200 psi | |
Lehmann & Voss LUVOCOM® 1105-8001 PEEK, with glass spheres Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Reduced moment of inertia compared with metal parts.Chemical and hydrolysis resistance par.. |
|||
Tensile Stress | 70.0 MPa | 10200 psi | |
Lehmann & Voss LUVOCOM® 1301-8060 PPS, linear, with glass fiber and PTFE, high viscosity Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Strong, stiff parts.Low warpage, isotropic shrinkage characteristics.Improved friction and wear be.. |