Polymer Property : Tensile Stress = 9.24 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 9.24 MPa

@Strain 100 %
1340 psi

@Strain 100 %
510 mm/min; ASTM D412A
PolyOne Elastamax™ XL-2165 Thermoplastic Polyolefin Elastomer (TPO (POE))
PolyOne's Elastamax™ XL thermoplastic olefins (TPOs) are based on pelletized blends of polyolefin resins and select elastomers such EPDM. These materials have been engineered to provide a balance o..