Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 9.03 MPa @Strain 100 % |
1310 psi @Strain 100 % |
Across Flow; ASTM D412 |
ExxonMobil Santoprene® 103-40 Thermoplastic Elastomer A hard, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range .. |
|||
Tensile Stress | 9.03 MPa @Strain 100 % |
1310 psi @Strain 100 % |
Across Flow; ASTM D412 |
ExxonMobil Santoprene® 203-40 Thermoplastic Elastomer A hard, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra.. |
|||
Tensile Stress | 9.03 MPa @Strain 100 % |
1310 psi @Strain 100 % |
Across Flow; ASTM D412 |
ExxonMobil Santoprene® 273-40 Thermoplastic Elastomer A hard, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as t.. |