Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 8.53 MPa @Strain 100 % |
1240 psi @Strain 100 % |
ASTM D412 |
Kolon ELLAS K-787A Ester Based Thermoplastic Polyurethane ApplicationsExtrusionInjectionFlexible HoseIndustry Parts Information provided by API-Kolon. |