Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 7.93 MPa @Strain 300 % |
1150 psi @Strain 300 % |
510 mm/min; ASTM D412A |
PolyOne Synprene™ RT-5190 RoHS Black Styrene Butadiene Block Copolymer (SBC) Synprene™ thermoplastic elastomers (TPEs) are compounds based on styrenic block copolymer (SBC) technology, and can be formulated to deliver extremely low hardness values not found in other elastom.. |
|||
Tensile Stress | 7.93 MPa @Strain 300 % |
1150 psi @Strain 300 % |
ASTM D412 |
Teknor Apex Telcar® TL-4145 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Tensile Stress | 7.93 MPa @Strain 100 % |
1150 psi @Strain 100 % |
ASTM D412 |
Teknor Apex Uniprene® UN-2467A Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |