Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 60.0 MPa | 8700 psi | |
Akro-Plastic Akromid® B4 S1 PA, Cold-Impact Resistant
(discontinued **) The outstanding characteristic is the reduction of the normally common cooling brittleness at low temperatures. Here, AKROMID A has set a course with special combinations like high heat stabilizatio.. |
|||
Tensile Stress | 60.0 MPa | 8700 psi | |
Lehmann & Voss LUVOCOM® 1301-7932 PPS, linear, with aramid reinforcement and PTFE Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Improved friction and wear behaviour. Emergency running property.Low warpage, isotropic shrinkage .. |
|||
Tensile Stress | 60.0 MPa | 8700 psi | |
Lehmann & Voss LUVOCOM® 20-7687 Polyphthalamide, with aramid reinforcement and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Low influence from moisture an.. |
|||
Tensile Stress | 60.0 MPa | 8700 psi | |
Lehmann & Voss LUVOCOM® 3/TF/20/BK Polyamide 6, with PTFE Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteristics.Reduce.. |
|||
Tensile Stress | 60.0 MPa | 8700 psi | |
Lehmann & Voss LUVOCOM® 3-8363 Polyamide 6, unreinforced Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteristics.Reduce.. |
|||
Tensile Stress | 60.0 MPa | 8700 psi | |
Lehmann & Voss LUVOCOM® 50-8479/BL Polycarbonate, unreinforced Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Isotropic shrinkage characteristics.Reduced moment of inertia .. |
|||
Tensile Stress | 60.0 MPa | 8700 psi | |
Lehmann & Voss LUVOCOM® 6-8512 Polyamide 12, with carbon fiber, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Especially suitable at dynamic.. |
|||
Tensile Stress | 60.0 MPa | 8700 psi | |
Lehmann & Voss LUVOCOM® 80-7666/GY Polyacetal-copolymer, with glass fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl.. |
|||
Tensile Stress | 60.0 MPa | 8700 psi | |
Lehmann & Voss LUVOCOM® NSB 90 NT Polyamide 66, with PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Tensile Stress | 60.0 - 70.0 MPa | 8700 - 10200 psi | ASTM D638 |
Iran Petrochemical (PCC) PC 0104 Polycarbonate Suitable for extrusionInformation provided by Iran Petrochemical Commercial Co. |
|||
Tensile Stress | 60.0 - 70.0 MPa | 8700 - 10200 psi | ASTM D638 |
Iran Petrochemical (PCC) PC 0407 Polycarbonate Suitable for extrusion, injection, and blow moldingInformation provided by Iran Petrochemical Commercial Co. |
|||
Tensile Stress | 60.0 - 70.0 MPa | 8700 - 10200 psi | ASTM D638 |
Iran Petrochemical (PCC) PC 1218 Polycarbonate Suitable for molding, injection, and blow moldingInformation provided by Iran Petrochemical Commercial Co. |
|||
Tensile Stress | 60.0 MPa | 8700 psi | |
Lehmann & Voss LUVOCOM® 1/GK/30/TF/13/SI/2 Polyamide 66, with glass spheres, PTFE, lubricant modified, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Low warpage, isotropic shrinka.. |
|||
Tensile Stress | 60.0 MPa | 8700 psi | |
Lehmann & Voss LUVOCOM® 1800-7432 PET, with PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Tensile Stress | 60.0 MPa | 8700 psi | |
Lehmann & Voss LUVOCOM® NSB 90 BK Polyamide 66, with PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Tensile Stress | 60.0 - 70.0 MPa | 8700 - 10200 psi | ASTM D638 |
Iran Petrochemical (PCC) PC 0712 Polycarbonate Suitable for molding and extrusionInformation provided by Iran Petrochemical Commercial Co. |
|||
Tensile Stress | 60.0 - 70.0 MPa | 8700 - 10200 psi | ASTM D638 |
Iran Petrochemical (PCC) PC 1822 Polycarbonate Suitable for injection moldingInformation provided by Iran Petrochemical Commercial Co. |