Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 150 MPa | 21800 psi | |
Lehmann & Voss LUVOCOM® 1105-7192 PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension.. |
|||
Tensile Stress | 150 MPa | 21800 psi | |
Lehmann & Voss LUVOCOM® 1105-8317/RD PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension.. |
|||
Tensile Stress | 150 MPa | 21800 psi | |
Lehmann & Voss LUVOCOM® 1105-8422 PEEK, with carbon fiber, PTFE, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; low thermal coefficient of expansion.Dynamic stressed parts at high m.. |
|||
Tensile Stress | 150 MPa | 21800 psi | |
Lehmann & Voss LUVOCOM® 1301-0793 PPS, linear, with glass fiber Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High-strength and stiff parts with low creep.High continuous use and heat distortion temperature. .. |
|||
Tensile Stress | 150 MPa | 21800 psi | |
Lehmann & Voss LUVOCOM® 19-7312/GN Polyamide 46, with glass fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Highly dimensionally stable at elevated temperatures.Gear parts for automot.. |
|||
Tensile Stress | 150 MPa | 21800 psi | |
Lehmann & Voss LUVOCOM® 19-7660 Polyamide 46, with glass fiber, PTFE, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Highly dimensionally stable at elevated temperatures.Gear parts for automot.. |
|||
Tensile Stress | 150 MPa | 21800 psi | |
Lehmann & Voss LUVOCOM® 20-7913 Polyphthalamide, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Low influence from moisture and temperature to measures and electrical prop.. |
|||
Tensile Stress | 150 MPa | 21800 psi | |
Lehmann & Voss LUVOCOM® 21-8115 Polyamide 6/6T, with carbon fiber, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Dynamic stressed parts at high movement velocity.Improved friction and wear.. |
|||
Tensile Stress | 150 MPa | 21800 psi | |
Lehmann & Voss LUVOCOM® 50/CF/10/GF/20/BK Polycarbonate, with carbon fiber and glass fiber Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi.. |
|||
Tensile Stress | 150 MPa | 21800 psi | |
Lehmann & Voss LUVOCOM® 50/CF/30 Polycarbonate, with carbon fiber Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi.. |
|||
Tensile Stress | 150 MPa | 21800 psi | |
Lehmann & Voss LUVOCOM® 1/GF/20/TF/10/SI/2/NC Polyamide 66, with glass fiber, PTFE, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Strong, stiff parts.Bearings, .. |
|||
Tensile Stress | 150 MPa | 21800 psi | |
Lehmann & Voss LUVOCOM® 1/GF/30/TF/15/BK Polyamide 66, with glass fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec.. |
|||
Tensile Stress | 150 MPa | 21800 psi | |
Lehmann & Voss LUVOCOM® 1105/GF/20/EM PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; impact resistance.Dynamic stressed parts at high movement velocity.Ch.. |
|||
Tensile Stress | 150 MPa | 21800 psi | |
Lehmann & Voss LUVOCOM® 1105-0904/GN PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.High dimensionally stable precision parts, high continuous use tempera.. |
|||
Tensile Stress | 150 MPa | 21800 psi | |
Lehmann & Voss LUVOCOM® 1105-7876-1 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Low warpage.Emergency running property.Information provided by Lehmann.. |
|||
Tensile Stress | 150 MPa | 21800 psi | |
Lehmann & Voss LUVOCOM® 1105-8184 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Low warpage.Emergency running property.Information provided by Lehmann.. |
|||
Tensile Stress | 150 MPa | 21800 psi | |
Lehmann & Voss LUVOCOM® 1-7956 Polyamide 66, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Electrically conductive.. |
|||
Tensile Stress | 150 MPa | 21800 psi | |
Lehmann & Voss LUVOCOM® 1850-7487 PBT, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricit.. |
|||
Tensile Stress | 150 MPa | 21800 psi | |
Lehmann & Voss LUVOCOM® 1/GF/20/TF/10/SI/2/BK Polyamide 66, with glass fiber, PTFE, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Strong, stiff parts.Bearings, .. |
|||
Tensile Stress | 150 MPa | 21800 psi | ISO 527-2 |
Solvay Specialty Polymers Ryton® R-4 Polyphenylene Sulfide (PPS), 40% Glass Fiber Ryton® R-4 and R-4-02 40% glass fiber reinforced polyphenylene sulfide compounds provide a good combination of mechanical and electrical properties with outstanding chemical resistance, even at e.. |
|||
Tensile Stress | 150 MPa | 21800 psi | |
Lehmann & Voss LUVOCOM® 1105-7173/BL PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension.. |