Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 130 MPa | 18900 psi | |
Lehmann & Voss LUVOCOM® 1105-7719/BN PEEK, with glass fiber, easy flowing Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension.. |
|||
Tensile Stress | 130 MPa | 18900 psi | |
Lehmann & Voss LUVOCOM® 1105-7760 PEEK, with carbon fiber, PTFE, lubricant modified, high viscosity Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; low thermal coefficient of expansion.Dynamic stressed parts at high m.. |
|||
Tensile Stress | 130 MPa | 18900 psi | |
Lehmann & Voss LUVOCOM® 1105-7776 PEEK, with carbon fiber, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Low warpage, isotropic shrinkage characteristics.Emergency running pro.. |
|||
Tensile Stress | 130 MPa | 18900 psi | |
Lehmann & Voss LUVOCOM® 1105-7828/GY PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension.. |
|||
Tensile Stress | 130 MPa | 18900 psi | |
Lehmann & Voss LUVOCOM® 1105-8108 PEEK, with glass fiber, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.Improved frict.. |
|||
Tensile Stress | 130 MPa | 18900 psi | |
Lehmann & Voss LUVOCOM® 1301/GF/30/TF/15 PPS, linear, with glass fiber and PTFE Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w.. |
|||
Tensile Stress | 130 MPa | 18900 psi | |
Lehmann & Voss LUVOCOM® 1301-8077 PPS, linear, with carbon fiber Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricity.S.. |
|||
Tensile Stress | 130 MPa | 18900 psi | |
Lehmann & Voss LUVOCOM® 1301-8456 PPS, linear, with glass fiber, PTFE, lubricant modified Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w.. |
|||
Tensile Stress | 130 MPa | 18900 psi | |
Lehmann & Voss LUVOCOM® 1301-8457 PPS, linear, with carbon fiber, lubricant modified Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.Strong, stiff parts.Suitable fo.. |
|||
Tensile Stress | 130 MPa | 18900 psi | |
Lehmann & Voss LUVOCOM® 1850/GF/30/TF/15/BK PBT, with glass fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec.. |
|||
Tensile Stress | 130 MPa | 18900 psi | |
Lehmann & Voss LUVOCOM® 1850-7783-1 PBT, with glass fiber, PTFE, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec.. |
|||
Tensile Stress | 130 MPa | 18900 psi | |
Lehmann & Voss LUVOCOM® 1850-8282 PBT, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricit.. |
|||
Tensile Stress | 130 MPa | 18900 psi | |
Lehmann & Voss LUVOCOM® 19-8263 Polyamide 46, with carbon fiber and glass fiber, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricit.. |
|||
Tensile Stress | 130 MPa | 18900 psi | |
Lehmann & Voss LUVOCOM® 3-7234-1 Polyamide 6, with carbon fiber, electrically conducting Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Strong, stiff parts.dynamic stressAntistatic.Handles, levers, rollers, body parts.Information provided by L.. |
|||
Tensile Stress | 130 MPa | 18900 psi | |
Lehmann & Voss LUVOCOM® 50-7844 Polycarbonate, with carbon fiber Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Strong, stiff parts; low thermal coefficient of expansion.Redu.. |
|||
Tensile Stress | 130 MPa | 18900 psi | |
Lehmann & Voss LUVOCOM® 80-7727 Polyacetal-copolymer, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; low thermal coefficient of expansion.Electrically conductive, suitable for.. |
|||
Tensile Stress | 130 MPa | 18900 psi | |
Lehmann & Voss LUVOCOM® 1105-7594/BL PEEK, with glass fiber, easy flowing Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension.. |
|||
Tensile Stress | 130 MPa | 18900 psi | |
Lehmann & Voss LUVOCOM® 1105-7720/BE PEEK, with glass fiber, easy flowing Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension.. |
|||
Tensile Stress | 130 MPa | 18900 psi | |
Lehmann & Voss LUVOCOM® 1800-7519 PET, with carbon fiber, PTFE, mineral resin Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and stiff parts with low creep.Electrically conductive, suitable for continuous d.. |
|||
Tensile Stress | 130 MPa | 18900 psi | |
Lehmann & Voss LUVOCOM® 1100-7890 Polyether sulfone, with carbon fiber Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.High dimensionally sta.. |
|||
Tensile Stress | 130 MPa | 18900 psi | ISO 527-2 |
Solvay Specialty Polymers Kalix® 2930 HFFR Polyamide, High Performance (HPPA), Glass Fiber Kalix® 2930 HFFR is a bio-sourced polyamide-based material specifically formulated to meet UL 94V2 @ 0.4 mm requirements for electronic devices. The material uses an advanced halogen-free flame r.. |
|||
Tensile Stress | 130 MPa | 18900 psi | |
Akro-Plastic Akromid® A3 GM 10/20 S1 PA, 10% Glass Filled, 20% Mineral Filled, Cold-Impact Resistant
(discont The outstanding characteristic is the reduction of the normally common cooling brittleness at low temperatures. Here, AKROMID A has set a course with special combinations like high heat stabilizatio.. |
|||
Tensile Stress | 130 MPa | 18900 psi | |
Lehmann & Voss LUVOCOM® 1301/CF/10/GF/20/GK/20/BK100 PPS, linear, with carbon fiber, glass fiber and micro glass spheres Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w.. |
|||
Tensile Stress | 130 MPa | 18900 psi | |
Lehmann & Voss LUVOCOM® 1-8130 Polyamide 66, with carbon fiber, aramid reinforcement and PTFE, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved wear behaviour, low warpage.Emergency running property, for highest tribologic needs.R.. |