Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 102 MPa | 14800 psi | ISO 527-2 |
Solvay Specialty Polymers Amodel® A-8422 LS WH159 Polyphthalamide (PPA), 22% Mineral Amodel® A-8422 LS is a light-stabilized, high-reflectivity, 22%-reinforced white polyphthalamide (PPA) that exhibits high heat resistance, high strength and stiffness over a broad temperature ran.. |