Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 450 - 600 MPa | 65300 - 87000 psi | |
ThyssenKrupp XABO® 355 Structural Steel This Material Specification applies to thermomechanically rolled flat products in thicknesses up to 60 mm. The criteria to distinguish the steel grades is the lowest test temperature for the notch-.. |
|||
Tensile Strength at Break | 300 - 600 MPa | 43500 - 87000 psi | |
Goodfellow Manganin® Copper Resistance Alloy Resistance alloy with moderate resistivity and low temperature coefficient. The resistance/temperature curve is not as flat as the constantans nor are the corrosion resistance properties as good.In.. |
|||
Tensile Strength at Break | 450 - 600 MPa | 65300 - 87000 psi | |
ThyssenKrupp XABO® 355 T Structural Steel This Material Specification applies to thermomechanically rolled flat products in thicknesses up to 60 mm. The criteria to distinguish the steel grades is the lowest test temperature for the notch-.. |