Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 49.0 - 54.0 MPa | 7110 - 7830 psi | ASTM D638 |
Solvay Specialty Polymers solvene® 250 EAP Electroactive Polymer (EAP) Annealing Temperature - < 135 °C; Breakdown Voltage - 250 kV/mm; Coercive Field - 50 kV/mm; Crystallization Point - ASTM D3418 123 °C; Curie Temperature - ASTM D3418 110 °C; d33 - -38.0 pC/.. |
|||
Tensile Strength at Break | 49.0 - 54.0 MPa | 7110 - 7830 psi | ASTM D638 |
Solvay Specialty Polymers solvene® T 2808 Electroactive Polymer (EAP) Annealing Temperature - < 135 °C; Breakdown Voltage - 250 kV/mm; Coercive Field - 50 kV/mm; Crystallization Point - ASTM D3418 123 °C; Curie Temperature - ASTM D3418 110 °C; d33 - -38.0 pC/.. |
|||
Tensile Strength at Break | 42.0 - 54.0 MPa | 6090 - 7830 psi | 5 mm/min.; IS 867-1963 |
Amity Thermosets ATG 116 Phenolic Molding Organic and inorganic Filler, Compression Molded Characteristics:Medium mechanical strength Medium electrical insulationGeneral purposeColor- BlackMedium flow Applications: Electrical accessories & fittings ( medium quality ) Domestic appliance ha.. |