Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 12.1 - 13.8 MPa | 1750 - 2000 psi | |
ITW Plexus Plexusâ„¢ MA1020 Methacrylate Adhesive Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Low shrinkage, low odor, all purpose.Information provided by Illinois Tool Works. |
|||
Tensile Strength at Break | 12.1 - 13.8 MPa | 1750 - 2000 psi | |
ITW Plexus Plexusâ„¢ MA1023 Methacrylate Adhesive Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Low shrinkage, low odor, all purpose.Information provided by Illinois Tool Works. |
|||
Tensile Strength at Break | 12.1 - 13.8 MPa | 1750 - 2000 psi | |
ITW Plexus Plexusâ„¢ MA1025 Methacrylate Adhesive Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Low shrinkage, low odor, able to be used 1" thick.Information provided by Illinois Tool Works. |
|||
Tensile Strength at Break | 12.1 - 13.8 MPa | 1750 - 2000 psi | |
ITW Plexus Plexusâ„¢ MA550 Methacrylate Adhesive Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Excellent marine adhesive, UV stable.Information provided by Illinois Tool Works. |